Category: | PP+EPDM , Polypropylene + EPDM Rubber |
Manufacturer: | Elastómeros Riojanos S.A. |
Trademark: | TPV Elastoprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ihqIzK_TPVElastopreneN73AE01.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
NE Series - TPV Elastoprene® It is a mixture of polypropylene and dynamically vulcanised EPDM rubber (PP/EPDM), with properties similar to those of other rubber products but with better results than traditional plastic materials. It has good resistance to the effects of ozone, UV rays and diverse chemical products, with an operating temperature of up to 135°C. It comes in pellet form, and it is transformed by means of traditional machinery used for plastic. It is a completely recyclable and reusable material. Recommended for extrusion and co-extrusion transformation processes |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ISO 1183/A |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shao A, 5 seconds, 6.00mm, extruded) | 73 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1(100% Strain, 2.00 mm) | 3.00 | MPa | ISO 37 |
Tensile Stress 2(Yield, 2.00 mm) | 7.00 | MPa | ISO 37 |
Tensile Elongation 3(Break, 2.00 mm) | 350 | % | ISO 37 |
Tear Strength 4(23°C, 2.00 mm) | 9.0 | kN/m | ISO 34-1 |
Compression Set 5(70°C, 22 hr) | 38 | % | ISO 815 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -58.0 | °C | ISO 812 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (2.0 mm) | HB | UL 94 |
Additional Information | Nominal Value | Test Method | |
---|---|---|---|
Ozone Resistance | 0 Rating | ISO 1431-1 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80 | °C | |
Melt Temperature | 170 - 200 | °C | |
Die Temperature | 200 - 220 | °C |
Note Message | |
---|---|
1 . | 500 mm/min |
2 . | 500 mm/min |
3 . | 500 mm/min |
4 . | Method A, Pant-Shaped Specimen |
5 . | Type a |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Utomer UT370 | Shanghai Utomer Material Science Co., Ltd. | TPU-Polyester | Utomer |
NEXUS PC/ABS PC/ABSQX7002 | Nexus Resin Group, LLC. | PC+ABS | NEXUS PC/ABS |
Celcon® GC25TF | Celanese Corporation | Acetal (POM) Copolymer | Celcon® |
EdgeGlas® TP | Plastic Selection Group, Inc. | TP, Unspecified | EdgeGlas® |
Osterlene® PPH-20-.5 | Osterman & Company | PP Homopolymer | Osterlene® |