Monprene® WR-12157 XRD

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Monprene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: iXGN1l_Monprene-WR-12157-XRD.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Monprene®WR-12157 XRD is a thermoplastic elastomer (TPE) material,. This product is available in North America, Africa and the Middle East, Latin America, Europe or Asia Pacific. The processing method is extrusion or injection molding.

Typical application areas include:
  • Handle
  • safety equipment
  • packing
  • kitchen utensils
  • engineering/industrial accessories
General Information
Uses
  • Safety equipment
  • Handle
  • Packaging
  • Kitchen utensils
  • Washer
  • Pipe fittings
  • Sporting goods
  • Shell
  • Stationery
  • Consumer goods application field
  • Toothbrush handle
  • Medical/nursing supplies
Appearance
  • Opacity
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.888g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (190°C/2.16 kg)8.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A, 1 sec 60ASTM D2240
    Shaw A, 5 seconds 57ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress (300% Strain)2.34MPaASTM D412
Tensile Strength (Break)7.93MPaASTM D412
Tensile Elongation (Break)680%ASTM D412
InjectionNominal ValueUnit
Rear Temperature 182 - 232°C
Middle Temperature 188 - 238°C
Front Temperature 193 - 243°C
Nozzle Temperature 199 - 249°C
Processing (Melt) Temp 199 - 249°C
Mold Temperature 35.0 - 48.9°C
Injection Pressure 1.38 - 5.52MPa
Injection Rate Fast
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 182 - 232°C
Cylinder Zone 2 Temp. 188 - 238°C
Cylinder Zone 3 Temp. 193 - 243°C
Cylinder Zone 5 Temp. 199 - 249°C
Die Temperature 199 - 249°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Resin Grade Manufacturer Category Trademark
PVC Film 165 D NT Teknor Apex Company PVC, Flexible PVC Film
Nycast 612VS C-90 Cast Nylons Ltd. Nylon 612 Nycast
Anjacom® 100V Almaak International GmbH PC Anjacom®
EL-Lene™ M735RU SCG Chemicals Co., Ltd. LLDPE EL-Lene™
LEXAN™ 925U resin SABIC Innovative Plastics PC LEXAN™