| Category: | PVC, Unspecified , Polyvinyl Chloride |
| Manufacturer: | Sylvin Technologies Incorporated |
| Trademark: | Sylvin |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | iEEzFa_Sylvin80288Green3185.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Sylvin 802-88 Green 3185 Is A Vinyl Compound Formulated For Profile Extrusion Applications. This Compound Meets The Requirements Of UL Sublect 1581, 720 Hour Sunlight Resistance Test. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.25 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness | ASTM D2240 | ||
| Shaw A | 88 | ASTM D2240 | |
| Shaw A, 10 seconds | 88 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 18.6 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 340 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength | 78.8 | kN/m | ASTM D624 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -27.0 | °C | ASTM D746 |
| Melting Temperature | 171 - 182 | °C |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Oxygen Index | 24 | % | ASTM D2863 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 4603 HI FR | RTP Company | SPS | RTP |
| Evoprene™ 047 | AlphaGary | SBS | Evoprene™ |
| Hostacom HBG H01 NAT | LyondellBasell Industries | PP Homopolymer | Hostacom |
| INNOPOL® PP CS 1-2110 AB | Inno-Comp Ltd. | PP Homopolymer | INNOPOL® PP |
| SQUARE® LSR2034-55BS | Shenzhen SQUARE Silicone Co., Ltd. | Silicone Rubber, LSR | SQUARE® |