Category: | EVA , Ethylene Vinyl Acetate Copolymer |
Manufacturer: | Horda Cable Compounds |
Trademark: | Horda |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | i8ewN2_HordaE8406.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Easy Strippable Semiconductive Shielding E8406 is a vulcanzisable, easy-strippable semiconductive compound, designed for both XLPE and EPDM rubber insulated cables and use in both dry and steam curing processes. E8406 meets the requirements as below, when optimal processing extrusion and end testing procedure are used: AEIC-CS 5/94 IEC 840 BS 6622 NF CS 32/321 HN 33-S-23 (EDF) SS 424 14 16, SS424 14 17 (HD 620 S1:1996) IEC 502 VDE 0273 / 12.87 |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.21 | g/cm³ | ASTM D1928 |
Moisture Content 1 | ppm | Internal method |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Thermoset 2(200°C) | 50 - 70 | % | IEC 60540 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 85 - 90 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | 13.0 | MPa | ASTM D638 |
Tensile Elongation (Break) | 240 | % | ASTM D638 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (135°C, 168 hr) | -5.0 | % | ASTM D638 |
Change in Ultimate Elongation in Air (135°C, 168 hr) | -25 | % | ASTM D638 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Volume Resistivity | ASTM D257 | ||
23°C | < 5.0E+2 | ohms·cm | ASTM D257 |
90°C | < 1.0E+3 | ohms·cm | ASTM D257 |
120°C | < 1.0E+3 | ohms·cm | ASTM D257 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | < 40 | °C | |
Cylinder Zone 1 Temp. | 60 - 110 | °C | |
Cylinder Zone 2 Temp. | 60 - 110 | °C | |
Cylinder Zone 3 Temp. | 60 - 110 | °C | |
Cylinder Zone 4 Temp. | 60 - 110 | °C | |
Cylinder Zone 5 Temp. | 60 - 110 | °C | |
Die Temperature | 100 - 130 | °C |
Extrusion instructions |
---|
Screw cooling: 40 to 50 °C |
Note Message | |
---|---|
1 . | QAHC-10420 (Karl Fischer method) |
2 . | 20 N/cm² |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
ADENE NCJBG | A.D. Compound spa | PP Copolymer | ADENE |
Exxelor™ VA 1840 | ExxonMobil Chemical | TP, Unspecified | Exxelor™ |
KOPHOS® KO1375 | Kolon Plastics, Inc. | PC | KOPHOS® |
ISPLEN® PP 040 G1E | REPSOL | PP Homopolymer | ISPLEN® |
ESTOPLAST EP 4030GY01 | Ester Industries Ltd. | PBT | ESTOPLAST EP |