| Category: | Fluorelastomer , Fluoroelastomer |
| Manufacturer: | Asahi Glass Co., Ltd. |
| Trademark: | AFLAS® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | holGlg_AFLAS-100H.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Commercial polymers are classified into two types; one is the TFE-P dipolymer type (AFLAS® 100/150 Series), and the other is the TFE-P-VdF terpolymer type (AFLAS® 200Series). AFLAS® 200 Series is characterized by the improved low temperature properties, demoldability and metal bonding while maintaining most of the high heat and chemical resistance and electrical resistivity of the dipolymer. Below the current polymer grades are listed, which are mainly classified according to Mooney viscosity. Dipolymer is mostly used in the wire and cable, and automotive industries, while terpolymer is often favored for automotive use in terms of processability. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Specific Gravity | 1.55 | g/cm³ | |
| Fluorine Content | 57 | % |
| Thermal | Nominal Value | Unit | |
|---|---|---|---|
| Glass Transition Temperature | -3.00 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Sindustris PBT TE5001HZ | Sincerity Australia Pty Ltd. | PC+PBT | Sindustris PBT |
| STERLENE™ CMV207E | R&P (Pte.) Ltd. | TPO (POE) | STERLENE™ |
| INLUBE PCGF10TF15 | Infinity LTL Engineered Compounds | PC | INLUBE |
| Karina WHITE PVC COMPOUND 752D10/151-B-IS | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |
| Optimum® 800 MF | RAUH Polymers, Inc. | Copolyester | Optimum® |