| Category: | TPC-ET , THERMOPLASTIC POLYESTER ELASTOMER |
| Manufacturer: | DuPont Performance Polymers |
| Trademark: | Hytrel® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | hGvGgn_Hytrel-SC988-NC010.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 82 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry |
| General Information | |
|---|---|
| Additive |
|
| Uses |
|
| Forms |
|
| Processing Method |
|
| Part Marking Code (ISO 11469) |
|
| Resin ID (ISO 1043) |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.28 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore D) | 82 | ISO 868 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 1180 | MPa | ISO 527-2 |
| Tensile Stress (Break) | 50.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | > 300 | % | ISO 527-2 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 15 | kJ/m² | ISO 179/1eA |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Melting Temperature 1 | 221 | °C | ISO 11357-3 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Wellamid® GFT13-66 XE-N | Wellman Engineering Resins | Nylon 66 | Wellamid® |
| Tru-Bond™ DC 200 | Devcon | Acrylic, Unspecified | Tru-Bond™ |
| Evermore PUR SS-1080HR | Evermore Chemical Industry Co., Ltd. | PUR, Unspecified | Evermore PUR |
| DJSilicone NE-9430 | DONGJUE SILICONE (NANJING) CO., LTD | Silicone | DJSilicone |
| LUVOCOM® 1301/CF/20 | LEHVOSS Group | PPS | LUVOCOM® |