| Category: | Nylon 12 , Polyamide 12 |
| Manufacturer: | Arkema |
| Trademark: | Rilsan® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | h7MHwp_Rilsan-MA-4430.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Rilsan® MA 4430 is a Polyamide 12 (Nylon 12) product. It can be processed by extrusion, injection molding, or profile extrusion and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1010 | 1010 | kg/m³ | ISO 1183 1 |
| Water Absorption | ISO 62 2 | |||
| Saturation | 1.2 | -- | % | |
| Equilibrium | 0.60 | -- | % |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile modulus | 530 | 490 | MPa | ISO 527-2 3 |
| Tensile Stress (Yield) | 31.0 | 29.0 | MPa | ISO 527-2 4 |
| Tensile Strain (Yield) | 22 | 23 | % | ISO 527-2 5 |
| Nominal strain at break | > 50 | > 50 | % | ISO 527-2 6 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy notched impact strength | ISO 179/1eA 7 | |||
| -30°C | 6.00 | 10.0 | kJ/m² | |
| 23°C | 75.0 | 100 | kJ/m² | |
| Charpy impact strength | ISO 179/1eU 8 | |||
| -30°C | No Break | No Break | ||
| 23°C | No Break | No Break |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Melting Temperature 9 | 175 | -- | °C | ISO 11357-3 10 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface resistivity | -- | 7.0E+14 | ohms | IEC 60093 11 |
| Volume resistivity | 1.0E+11 | 1.0E+11 | ohms·m | IEC 60093 12 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 13 | |
| Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 14 | |
| Oxygen index | 20 | -- | % | ISO 4589-2 15 |
| Note Message | |
|---|---|
| 1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 9 . | 10 °C/min |
| 10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| 15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| XYRON™ X531Z | Asahi Kasei Chemicals Corporation | PPE+PS | XYRON™ |
| ADENE NCJE | A.D. Compound spa | PP Homopolymer | ADENE |
| Plaslube® ABS 8005 | Techmer Engineered Solutions | ABS | Plaslube® |
| ESTOPLAST XU 6250BB10 | Ester Industries Ltd. | Nylon 66 | ESTOPLAST XU |
| Moplen EP545L | LyondellBasell Industries | PP Impact Copolymer | Moplen |