Category: | PEBA-Ether , Polyether Block Amide |
Manufacturer: | Arkema |
Trademark: | Pebax® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gycpdE_Pebax-5533-SN-70-NOIR.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Pebax® 5533 SN 70 NOIR is a Polyether Block Amide (PEBA-Ether) product filled with filler. It can be processed by blow molding, calendering, casting, coating, extrusion, film extrusion, injection molding, profile extrusion, resin transfer molding, sheet extrusion, or thermoforming and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1090 | 1090 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (250°C/5.0 kg) | 5.00 | -- | cm³/10min | ISO 1133 2 |
Water Absorption (Saturation) | 1.2 | -- | % | ISO 62 3 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 305 | 298 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 18.0 | 17.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 31 | 36 | % | ISO 527-2 6 |
Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 18.0 | -- | kJ/m² | |
23°C | No Break | -- | ||
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | No Break | -- | ||
23°C | No Break | -- |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Melting Temperature 10 | 159 | -- | °C | ISO 11357-3 11 |
CLTE - Flow | 2.2E-4 | -- | cm/cm/°C | ISO 11359-2 12 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface resistivity | -- | 5.5E+3 | ohms | IEC 60093 13 |
Volume resistivity | 1.1E+5 | -- | ohms·m | IEC 60093 14 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 15 | |
Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 16 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | 10 °C/min |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
HOPELEN J-150 | Lotte Chemical Corporation | PP Homopolymer | HOPELEN |
Lionpol HF-200223 | Lion Polymers Incorporated | TPE | Lionpol |
Lumid® GP2500B(W) | LG Chem Ltd. | Nylon 66 | Lumid® |
CALIBRE™ 301-40 | Sumika Styron Polycarbonate Limited | PC | CALIBRE™ |
POTICON RT8 | Otsuka Chemical Co., Ltd. | PPS | POTICON |