Category: | EVA , Ethylene Vinyl Acetate Copolymer Resin |
Manufacturer: | ExxonMobil Chemical |
Trademark: | Escorene™ Ultra |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | gxTKbw_Escorene-Ultra-LD-761-36.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Escorene Ultra LD 761.36 is a copolymer containing 26.7% vinyl acetate with excellent flexibility and low temperature toughness. LD 761.36 can accommodate high proportion of packing. |
General Information | |
---|---|
Additive |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Vinyl Acetate Content | 26.7 | wt% | ExxonMobil Method |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness | ASTM D2240 | ||
Shaw A, 15 seconds | 76 | ASTM D2240 | |
Shaw D, 15 seconds | 27 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength (Break) | 8.07 | MPa | ASTM D638 |
Tensile Elongation (Break) | > 800 | % | ASTM D638 |
Flexural Modulus - 1% Secant | 28.0 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Instrumented Dart Impact | ASTM D3763 | ||
-40°C | 29.8 | J | ASTM D3763 |
23°C | 19.0 | J | ASTM D3763 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Vicat Softening Temperature | 46.0 | °C | ASTM D1525 |
Legal statement |
---|
有关潜在食品接触应用合规信息(例如:FDA、EU、HPFB),请与埃克森美孚化工客户服务代表联系。本产品不宜在医疗应用中使用,亦不应在任何此类应用中使用 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MEGOLON™ S530 | AlphaGary | TP, Unspecified | MEGOLON™ |
TRANSMARE® BIO 35LANF30-0.101 | Transmare Compounding B.V. | PLA | TRANSMARE® BIO |
Amodel® FC-1140 | Solvay Specialty Polymers | PPA | Amodel® |
HIPOLEN P® MA 21 | HIPOL A.D. | PP Homopolymer | HIPOLEN P® |
Later 4-V0HF1 | LATI S.p.A. | PBT | Later |