Message |
---|
Glass fibre-reinforced Chemically coupled |
General Information | |
---|---|
Filler / Reinforcement |
|
Features |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.05 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 15 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.60 | % | |
Flow | 0.30 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 80.0 | MPa | ISO 527-2 |
Tensile Strain (Break) | 4.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 4500 | MPa | ISO 178 |
Flexural Stress | 110 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 3.0 | kJ/m² | |
23°C | 5.0 | kJ/m² |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 150 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 130 | °C | ISO 75-2/A |
Vicat Softening Temperature | 125 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
SEETEC EVA EF221 | LG Chem Ltd. | EVA | SEETEC EVA |
ALTECH® PA6 B 2030/500 GF30 | ALBIS PLASTIC GmbH | Nylon 6 | ALTECH® PA6 |
FERREX® GPP35CG40UL GRAY | Ferro Corporation | PP Homopolymer | FERREX® |
Interpol 47-5138/47-5205 20%Glass | Cook Composites and Polymers | PUR-Ester | Interpol |
OnFlex™ S FR 80A-3S1892 | PolyOne Corporation | TPE | OnFlex™ |