| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | Wellamid® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gVHDhQ_Wellamid-GS25-66-22L-NBK1.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Wellamid® GS25-66 22L-NBK1 is a Polyamide 66 (Nylon 66) material filled with 25% glass bead. It is available in Asia Pacific, Europe, Latin America, or North America. Primary attribute of Wellamid® GS25-66 22L-NBK1: Flame Rated. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Appearance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.32 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow | 1.5 to 1.9 | % | |
| Flow | 1.4 to 1.8 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield) | 70.0 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.0 | % | ISO 527-2 |
| Flexural Modulus | 3900 | MPa | ISO 178 |
| Flexural Stress | 114 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Unnotched Izod Impact Strength | 3.3 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 84.0 | °C | ISO 75-2/A |
| Melting Temperature | 260 | °C | ISO 3146 |
| Flammability | Nominal Value | Test Method | |
|---|---|---|---|
| Flame Rating (1.50 mm) | HB | UL 94 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| ELASTOSIL® LR 3071/60 A/B | Wacker Chemie AG | Silicone | ELASTOSIL® LR |
| KOPA® KN333G15BL | Kolon Plastics, Inc. | Nylon 66 | KOPA® |
| KOPELEN JI-360 | Lotte Chemical Corporation | PP Impact Copolymer | KOPELEN |
| ICORENE® N9602 | ICO Polymers EMEA, A Division of A. Schulman | Nylon 6 | ICORENE® |
| Hifax TRC 770P G64 Gray | LyondellBasell Industries | TPO (POE) | Hifax |