Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.23 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 20 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 0.80 to 1.0 | % | |
Flow | 0.80 to 1.0 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 26.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 5.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 2600 | MPa | ISO 178 |
Flexural Stress | 46.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength (23°C) | 5.0 | kJ/m² | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 110 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 70.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 142 | °C | ISO 306/A50 |
-- | 73.0 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 750 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sylvin 8200-55 Clear 876 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Aaroprene® CFIPP 2040 | Aaron Industries Corp. | PP, Unspecified | Aaroprene® |
ESTOPLAST XU 400 NN11 | Ester Industries Ltd. | Nylon, Unspecified | ESTOPLAST XU |
LUVOCOM® GS-58 | Lehmann & Voss & Co. | Nylon 66 | LUVOCOM® |
Kepamid® 1315GFH | Korea Engineering Plastics Co., Ltd | Nylon 6 | Kepamid® |