| Category: | Nylon 6 , Polyamide 6 |
| Manufacturer: | A. Schulman Europe |
| Trademark: | SCHULAMID® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gKWkS1_SCHULAMID-6-GF-35.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| 35% glass fiber reinforced Polyamide 6 |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Features |
|
| UL File Number |
|
| Processing Method |
|
| Resin ID (ISO 1043) |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.41 | -- | g/cm³ | ISO 1183/A |
| Viscosity Number | 145 | -- | cm³/g | ISO 307 |
| Hardness | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Ball Indentation Hardness (H 358/30) | 230 | -- | MPa | ISO 2039-1 |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 11000 | 7000 | MPa | ISO 527-2/1A/1 |
| Tensile Stress (Break) | 180 | 110 | MPa | ISO 527-2/1A/5 |
| Tensile Strain (Break) | 3.4 | 6.0 | % | ISO 527-2/1A/5 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | |||
| -30°C | 10 | -- | kJ/m² | |
| 23°C | 15 | 32 | kJ/m² | |
| Charpy Unnotched Impact Strength | ISO 179/1eU | |||
| -30°C | 70 | -- | kJ/m² | |
| 23°C | 90 kJ/m² | No Break |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, Unannealed | 220 | -- | °C | ISO 75-2/Bf |
| 1.8 MPa, Unannealed | 210 | -- | °C | ISO 75-2/Af |
| Vicat Softening Temperature | 210 | -- | °C | ISO 306/B50 |
| Ball Pressure Test (150°C) | Pass | -- | IEC 60695-10-2 |
| Electrical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Surface Resistivity | > 1.0E+15 | > 1.0E+12 | ohms | IEC 60093 |
| Volume Resistivity | > 1.0E+13 | > 1.0E+10 | ohms·cm | IEC 60093 |
| Comparative Tracking Index | 450 | -- | V | IEC 60112 |
| Flammability | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Burning Rate | < 100 | -- | mm/min | ISO 3795 |
| Flammability Classification | IEC 60695-11-10, -20 | |||
| 1.50 mm | HB | -- | ||
| 3.00 mm | HB | -- | ||
| Glow Wire Flammability Index | IEC 60695-2-12 | |||
| 1.50 mm | -- | 650 | °C | |
| 3.00 mm | -- | 650 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® C4905 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| Maxelast® P3991 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| SUNFROST® KD90EA | Mitsubishi Chemical Performance Polymers, Inc. | PVC Elastomer | SUNFROST® |
| Ultramid® 8262G HS BK-125 | BASF Corporation | Nylon 6 | Ultramid® |
| NYLOY® PG-0220B | Nytex Composites Co., Ltd. | PP, Unspecified | NYLOY® |