| Category: | TPO (POE) , Thermoplastic Polyolefin Elastomer |
| Manufacturer: | API SpA |
| Trademark: | apigo® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | gK53RB_apigo-9160-NL-60.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
apigo®9160 NL/60 is a polyolefin thermoplastic elastomer (TPO (POE)) product,. It can be processed by extrusion or injection molding and is available in Europe. apigo®9160 NL/60 applications include consumer goods, electrical appliances, engineering/industrial accessories, home applications and construction applications. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.09 | g/cm³ | ASTM D792 |
| Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 90 | g/10 min | ASTM D1238 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 60 | ASTM D2240 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | ASTM D638 | ||
| -- | 3.80 | MPa | ASTM D638 |
| 100% strain | 1.20 | MPa | ASTM D638 |
| 300% strain | 1.70 | MPa | ASTM D638 |
| Tensile Elongation (Break) | 650 | % | ASTM D638 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tear Strength 1 | 20.0 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 150 - 170 | °C | |
| Middle Temperature | 160 - 180 | °C | |
| Front Temperature | 170 - 190 | °C | |
| Nozzle Temperature | 180 - 200 | °C | |
| Injection Rate | Slow-Moderate |
| Injection instructions |
|---|
| Injection Pressure: HighBack Pressure: MediumLocking Pressure: High |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 150 - 180 | °C | |
| Cylinder Zone 2 Temp. | 160 - 190 | °C | |
| Cylinder Zone 3 Temp. | 170 - 190 | °C | |
| Cylinder Zone 4 Temp. | 180 - 190 | °C |
| Extrusion instructions |
|---|
| L/D Ratio: >20:1Compression Ratio: 1:2.5 to 1:3 |
| Note Message | |
|---|---|
| 1 . | Without Notch |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Chemlon® 104 H | Teknor Apex Company (Chem Polymer) | Nylon 66 | Chemlon® |
| Kelon® B FR H CETG/250-V0 | LATI S.p.A. | Nylon 6 | Kelon® B |
| ISPLEN® PM 275 AW | REPSOL | PP Copolymer | ISPLEN® |
| Leona™ FG171 | Asahi Kasei Chemicals Corporation | Nylon 66 | Leona™ |
| StarFlex® 7360-1000 | Star Thermoplastic Alloys & Rubbers, Inc. | TPE | StarFlex® |