Category: | Nylon 66 , Polyamide 66 |
Manufacturer: | Ravago Manufacturing Americas, LLC |
Trademark: | Hylon® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | g545HC_Hylon-N1243L.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Nylon 66, 43% Glass Filled |
General Information | |
---|---|
Filler / Reinforcement |
|
RoHS Compliance |
|
UL File Number |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 1.49 | g/cm³ | ISO 1183 |
Molding Shrinkage - Flow (3.18 mm) | 0.30 to 0.50 | % | ISO 294-4 |
Water Absorption (23°C, 24 hr) | 0.60 | % | ISO 62 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (M-Scale) | 103 | ISO 2039-2 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Break) | 183 | MPa | ISO 527-2 |
Tensile Strain (Break) | 2.0 | % | ISO 527-2 |
Flexural Modulus | 9650 | MPa | ISO 178 |
Flexural Stress | 248 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact Strength | 9.0 | kJ/m² | ISO 180 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (1.8 MPa, Unannealed) | 252 | °C | ISO 75-2/A |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (1.50 mm) | HB | UL 94 |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sanren EVA 12/0.5 | SINOPEC Shanghai Petrochemical Co. Ltd. | EVA | Sanren |
Solprene® 1110 | Dynasol Elastomers | SBR, Solution | Solprene® |
Spartech Polycom PP5240 | Spartech Polycom | PP Homopolymer | Spartech |
Titalon® 1300GB | Titan Plastics Compounds Co., Ltd. | Nylon 6 | Titalon® |
Karina GRAY PVC COMPOUND -E 843-18/302-CRM | Karina Ind. e Com. de Plásticos Ltda | PVC, Unspecified | Karina |