| Category: | TPE , Thermoplastic Elastomer |
| Manufacturer: | Mitsubishi Chemical Performance Polymers, Inc. |
| Trademark: | THERMORUN® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | g1C8Av_THERMORUN-3555B-N.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| THERMORUN®3555B/N is a thermoplastic elastomer (TPE) material,. This product is available in North America, Europe or Asia Pacific. The processing method is extrusion or injection molding. THERMORUN®The main characteristics of 3555B/N are: low hardness. |
| General Information | |
|---|---|
| Features |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.880 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (230°C/5.0 kg) | 2.0 | g/10 min | ISO 1133 |
| Molding Shrinkage | ISO 294-4 | ||
| Vertical flow direction | 1.5 - 2.0 | % | ISO 294-4 |
| Flow direction | 1.5 - 2.0 | % | ISO 294-4 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 55 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress | ISO 37 | ||
| 100% strain | 1.60 | MPa | ISO 37 |
| 300% strain | 2.80 | MPa | ISO 37 |
| Tensile Stress (Break) | 6.00 | MPa | ISO 37 |
| Tensile Elongation (Break) | 600 | % | ISO 37 |
| Tear Strength | 28 | kN/m | ISO 34-1 |
| Compression Set (70°C, 22 hr) | 35 | % | ISO 815 |
| Additional Information |
|---|
| Data obtained using JIS test methods. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 2103 TFE 15 | RTP Company | PEI | RTP |
| APEX® 2580-H | Teknor Apex Company | PVC, Flexible | APEX® |
| Elastocon® OF75 | Elastocon TPE Technologies | TPE | Elastocon® |
| Resilience™ LS21040M | PolyOne Corporation | PVC, Rigid | Resilience™ |
| Chemlon® 904-13 GVNH | Teknor Apex Company (Chem Polymer) | Nylon, Unspecified | Chemlon® |