Category: | Unspecified , Unspecified |
Manufacturer: | Eastman Chemical Company |
Trademark: | Amphora™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | fzCCfM_Amphora3DPolymerHT5300.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Eastman Amphora™ HT5300 3D polymer is a low-odor, and styrene-free material uniquely suited for advanced 3D printing users, particularly those who need their creations to exhibit superior durability, dimensional stability, toughness, and high temperature resistance.The model of functional aesthetics, Amphora HT5300 can be made into high-quality filament that exhibits advanced overhang ability, excellent toughness and temperature resistance, good looks, and superior melt strength—empowering professional users to create durable, more useful items. Demonstrating superior dimensional stability, BPA-free HT5300 allows for 3D printing to exacting dimensions, which is especially important for products with tight tolerances and multi-component parts. Moreover, with its outstanding toughness and chemical resistance, Amphora HT5300 is ideal for prototyping and testing products, especially for applications that require temperature resistance up to 100°C. |
General Information | |
---|---|
Features |
|
Uses |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.18 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Rockwell Hardness (R-Scale, 23°C) | 111 | ASTM D785 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Strength | ASTM D638 | ||
Yield, 23°C | 43.0 | MPa | ASTM D638 |
Fracture, 23°C | 52.0 | MPa | ASTM D638 |
Tensile Elongation | ASTM D638 | ||
Yield, 23°C | 7.0 | % | ASTM D638 |
Fracture, 23°C | 210 | % | ASTM D638 |
Flexural Modulus (23°C) | 1580 | MPa | ASTM D790 |
Flexural Strength | 64.0 | MPa | ASTM D790 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Notched Izod Impact (23°C) | 860 | J/m | ASTM D256 |
Unnotched Izod Impact (23°C) | No Break | ASTM D4812 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Deflection Temperature Under Load | ASTM D648 | ||
0.45 MPa, not annealed | 94.0 | °C | ASTM D648 |
1.8 MPa, not annealed | 81.0 | °C | ASTM D648 |
Additional Information |
---|
Typical Processing Conditions: Processing Melt Temperature: 250 to 260°C Heated Bed Temperature: 90 to 110°C Cooling: 0 to 100% Layer Height: 0.1 or 0.2 mm Speed: 30 to 600 mm/s Infill: As needed up to 100% Perimeter: Around 1 mm Minimal Layer Time: 5 sec |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 200 F TFE 15 | RTP Company | Nylon 12 | RTP |
APEX® 87-L701-D | Teknor Apex Company | PVC, Flexible | APEX® |
HOPELEN FR-170 | Lotte Chemical Corporation | PP Homopolymer | HOPELEN |
Plaslube® PPS GF30 SL2 | Techmer Engineered Solutions | PPS | Plaslube® |
Sylvin 9791-75UV Black | Sylvin Technologies Incorporated | PVC, Flexible | Sylvin |