| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Polykemi AB |
| Trademark: | SCANAMID 66 |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | fmgDN4_SCANAMID-66-A12-F30-TF15.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Glass fibre reinforced, modified |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.49 | -- | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | |||
| Across Flow | 1.1 | -- | % | |
| Flow | 0.30 | -- | % |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Stress | 165 | 125 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 4.0 | 6.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 8100 | 4800 | MPa | ISO 178 |
| Flexural Stress | 230 | 148 | MPa | ISO 178 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 10 | -- | kJ/m² | ISO 179 |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature 1 | ||||
| 0.45 MPa, Unannealed | 250 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 250 | -- | °C | ISO 75-2/A |
| Vicat Softening Temperature | > 230 | -- | °C | ISO 306/B50 |
| Note Message | |
|---|---|
| 1 . | 120°C/hr |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Thermylene® P7-40FG-0600 | Asahi Kasei Plastics North America Inc. | PP, Unspecified | Thermylene® |
| ACCUCOMP™ LD0102L | ACLO Compounders Inc. | LDPE | ACCUCOMP™ |
| DuraGrip® DGR 6240TR | Advanced Polymer Alloys | TPE | DuraGrip® |
| Envirez® MR 56301 | Ashland Performance Materials | Polyester, TS | Envirez® |
| Hostacom PPU X9067HS G62490 | LyondellBasell Industries | PP Copolymer | Hostacom |