| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Teknor Apex Company (Chem Polymer) |
| Trademark: | Chemlon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | fhg0lV_Chemlon-150-GHU.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Chemlon® 150 GHU is a Polyamide 66 (Nylon 66) material filled with glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Primary attribute of Chemlon® 150 GHU: Flame Rated. |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.56 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow 1 | 0.070 to 0.17 | % | ASTM D955 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength | 228 | MPa | ASTM D638 |
| Tensile Elongation | ASTM D638 | ||
| Yield | 2.0 | % | |
| Break | 2.0 | % | |
| Flexural Modulus | 13400 | MPa | ASTM D790 |
| Flexural Strength | 309 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (23°C) | 190 | J/m | ASTM D256 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | > 255 | °C | ASTM D648 |
| Melting Temperature | 261 | °C | ASTM D789 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Volume Resistivity | 1.0E+15 | ohms·cm | ASTM D257 |
| Dielectric Strength (3.00 mm) | 16 | kV/mm | ASTM D149 |
| Dielectric Constant (1 MHz) | 3.90 | ASTM D150 | |
| Comparative Tracking Index (CTI) | 600 | V | UL 746 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.810 mm) | HB | UL 94 | |
| Oxygen Index | 25 | % | ASTM D2863 |
| FMVSS Flammability | Passed | FMVSS 302 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 79.4 | °C | |
| Suggested Max Moisture | 0.20 | % | |
| Suggested Max Regrind | 25 | % | |
| Rear Temperature | 252 to 279 | °C | |
| Middle Temperature | 268 to 291 | °C | |
| Front Temperature | 268 to 291 | °C | |
| Nozzle Temperature | 268 to 291 | °C | |
| Processing (Melt) Temp | 266 to 285 | °C |
| Note Message | |
|---|---|
| 1 . | Dependent upon molding conditions particularly Mold temperature. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Alpha PVC GEX 03-040 F NATURAL | AlphaGary | PVC, Flexible | Alpha PVC |
| ASTAPET™ PC/PET MDA267 | Marplex Australia Pty. Ltd. | PET | ASTAPET™ |
| Hostacom G2 U42 L356015 | LyondellBasell Industries | PP Homopolymer | Hostacom |
| TECACOMP® PPA LDS black 4109 | Ensinger GmbH | PPA | TECACOMP® |
| Kepital® ES-20 | KEP Americas | Acetal (POM) Copolymer | Kepital® |