| Starflam PF0057E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1005Z270) |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Additive |
|
| Features |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.39 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 24 hr | 0.90 to 1.3 | % | |
| Flow : 24 hr | 0.10 to 0.30 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 9500 | MPa | ISO 527-2/1 |
| Tensile Stress (Break) | 145 | MPa | ISO 527-2 |
| Tensile Strain (Break) | 3.0 | % | ISO 527-2 |
| Flexural Modulus | 8000 | MPa | ISO 178 |
| Flexural Stress | 210 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength 1(23°C) | 10 | kJ/m² | ISO 180/1A |
| Unnotched Izod Impact Strength 2(23°C) | 54 | kJ/m² | ISO 180/1U |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 3(1.8 MPa, Unannealed, 64.0 mm Span) | 205 | °C | ISO 75-2/Af |
| Ball Pressure Test 4(200°C) | Pass | IEC 60695-10-2 | |
| Thermal Conductivity | 0.30 | W/m/K | ISO 8302 |
| RTI Elec | 140 | °C | UL 746 |
| RTI Imp | 105 | °C | UL 746 |
| RTI Str | 140 | °C | UL 746 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Comparative Tracking Index | 600 | V | IEC 60112 |
| High Amp Arc Ignition (HAI) | PLC 0 | UL 746 | |
| Hot-wire Ignition (HWI) | PLC 0 | UL 746 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating (0.800 mm) | V-0 | UL 94 | |
| Glow Wire Flammability Index (0.800 mm) | 960 | °C | IEC 60695-2-12 |
| Glow Wire Ignition Temperature | IEC 60695-2-13 | ||
| 1.00 mm | 775 | °C | |
| 1.50 mm | 775 | °C | |
| 3.00 mm | 800 | °C |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 80.0 | °C | |
| Drying Time | 4.0 | hr | |
| Suggested Max Moisture | 0.20 | % | |
| Rear Temperature | 240 to 250 | °C | |
| Middle Temperature | 250 to 260 | °C | |
| Front Temperature | 250 to 270 | °C | |
| Processing (Melt) Temp | 250 to 270 | °C | |
| Mold Temperature | 50.0 to 90.0 | °C |
| Note Message | |
|---|---|
| 1 . | 80*10*4 |
| 2 . | 80*10*4 |
| 3 . | 80*10*4 |
| 4 . | Approximate maximum |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Tecomid® NB40 KG30 NL 0G | Eurotec Engineering Plastics | Nylon 6 | Tecomid® |
| Moplen HP623J | PolyMirae | PP Homopolymer | Moplen |
| Nucrel® 31001 | DuPont Packaging & Industrial Polymers | EAA | Nucrel® |
| Delrin® 327UVE RD402 | DuPont Performance Polymers | Acetal (POM) Homopolymer | Delrin® |
| Kingfa JH-R2G10 P60 | Kingfa | PC+ABS | Kingfa |