RTP 1505-55D

Category: TEEE , Thermoplastic Elastomer, Ether-Ester
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: ffaiza_RTP-1505-55D.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 30% filler by weight
RoHS Compliance
  • Contact manufacturer
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.42g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.15 - 0.21%ASTM D955
Moisture Content %
Additional InformationNominal ValueUnit
Primary Additive 30%
HardnessNominal ValueUnitTest Method
Durometer Hardness (Shore D)65ASTM D2240
MechanicalNominal ValueUnitTest Method
Tensile Modulus 2480MPaASTM D638
Tensile Strength 50.7MPaASTM D638
Tensile Elongation (Yield)9.2%ASTM D638
Flexural Modulus 2340MPaASTM D790
Flexural Strength 70.3MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)360J/mASTM D256
Unnotched Izod Impact (3.20 mm)No BreakASTM D4812
InjectionNominal ValueUnit
Drying Temperature 104°C
Drying Time 2.0 - 4.0hr
Processing (Melt) Temp 210 - 238°C
Mold Temperature 21.1 - 37.8°C
Injection Pressure 68.9 - 103MPa
Injection instructions
Desiccant Type Dryer Required.
Resin Grade Manufacturer Category Trademark
Toler PP 9038N Toler Chemical, Inc PP Homopolymer Toler PP
Cellidor B 531-10 ALBIS PLASTIC GmbH CAB Cellidor
Polybutene-1 PB 0110M LyondellBasell Industries PB Polybutene-1
Polygen SG6C-BK Shanghai Polygen Science and Technology Co., Ltd. PPS Polygen
Sylvin 86042-75 Clear 8422 Sylvin Technologies Incorporated PVC, Unspecified Sylvin