Hifax TRC 835P LAH DARK GREY high melt flow, medium high flexural modulus, precolored, UV-stabilized, mineral filled, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of properties. It is typically used for automotive exterior trim applications. For regulatory compliance information, see Hifax TRC 835P LAH DARK GREY Product Stewardship Bulletin (PSB) and Safety Data Sheet (SDS). |
General Information | |
---|---|
Filler / Reinforcement |
|
Additive |
|
Features |
|
Uses |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density (23°C) | 1.03 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 38 | g/10 min | ASTM D1238 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (Yield, 23°C) | 19.5 | MPa | ISO 527-2 |
Tensile Strain (Yield, 23°C) | 8.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 1800 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Instrumented Dart Impact (-15°C, Ductile Failure) | 26.0 | J | ASTM D3763 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature (0.45 MPa, Unannealed) | 90.0 | °C | ISO 75-2/B |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Prime ABS PC/ABS | Primex Plastics Corporation | PC+ABS | Prime ABS |
TPV Elastoprene® N40D-S | ELASTORSA Elastomeros Riojanos S.A. | PP+EPDM | TPV Elastoprene® |
TOTAL Polypropylene PPH 3866 | TOTAL Refining & Chemicals | PP Homopolymer | TOTAL Polypropylene |
Varcum 29738 | Durez Corporation | Phenolic | Varcum |
ULTEM™ 2212R resin | SABIC Innovative Plastics | PEI | ULTEM™ |