Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Nantex Industry Co., Ltd. |
Trademark: | Dynaprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | fLmk0w_Dynaprene-VE0064A.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Dynaprene® VE0064A is a Thermoplastic Elastomer (TPE) material. It is available in Asia Pacific for injection molding. |
General Information | |
---|---|
Features |
|
Uses |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 0.958 | g/cm³ | ASTM D792 |
Moisture Content | < 0.060 | % | Internal Method |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 66 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Set (100% Strain) | 11 | % | ASTM D412 |
Tensile Stress (100% Strain) | 2.30 | MPa | ASTM D412 |
Tensile Strength - Across Flow (Yield) | 5.80 | MPa | ASTM D412 |
Tensile Elongation - Across Flow (Break) | 380 | % | ASTM D412 |
Tear Strength 1(23°C) | 34.0 | kN/m | ASTM D624 |
Compression Set (100°C, 22 hr) | 28 | % | ASTM D395B |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Volume (121°C, 24 hr, in IRM 903 Oil) | 77 | % | ASTM D471 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | < -60.0 | °C | ASTM D746 |
Note Message | |
---|---|
1 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
TEKNIFLEX® MED 3014-0180 | Tekni-Films, a div of Tekni-Plex | Film, PP | TEKNIFLEX® MED |
Kepital® TE-21 | Korea Engineering Plastics Co., Ltd | Acetal (POM) Copolymer | Kepital® |
HydroMed™ D4 | AdvanSource Biomaterials Corp. | PUR-Ether | HydroMed™ |
KEBAFLEX® E D 50.1 | BARLOG plastics GmbH | TPV | KEBAFLEX® |
Sylvin 8225-65FUV Black | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |