Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | Miracll Chemicals Co., Ltd. |
Trademark: | Mirathane™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | eh8Pgh_Mirathane-E175D.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Mirathane™ E175D is a Thermoplastic Polyurethane Elastomer (Polyester) (TPU-Polyester) product. It is available in Asia Pacific. Applications of Mirathane™ E175D include coating applications, engineering/industrial parts, hose/tubing, additive/masterbatch and automotive. Characteristics include:
|
General Information | |
---|---|
Features |
|
Uses |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.22 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 73 to 75 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Abrasion Loss | 40.0 | mm³ | DIN 53516 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 30.0 to 35.0 | MPa | |
300% Strain | 43.0 | MPa | |
Tensile Strength (Yield) | 41.0 to 50.0 | MPa | ASTM D412 |
Tensile Elongation (Break) | 250 to 300 | % | ASTM D412 |
Tear Strength | 240 to 260 | kN/m | ASTM D624 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature 1 | -20.0 | °C | ASTM D3417 |
Note Message | |
---|---|
1 . | 10°C/min |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 204 A FR | RTP Company | Nylon 6 | RTP |
Sanren F850EBA (Premium-grade) | SINOPEC Shanghai Petrochemical Co. Ltd. | PP Homopolymer | Sanren |
AKROMID® B28 GF 50 1 GIT black (5649) | AKRO-PLASTIC GmbH | Nylon 6 | AKROMID® |