Category: | TPU-Polyester , Thermoplastic Polyurethane Elastomer (Polyester) |
Manufacturer: | BASF Corp. Thermoplastic Polyurethanes |
Trademark: | Elastollan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | eBR6Wc_Elastollan-S85AN.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Elastollan® S85AN is specifically formulated for injection molding applications with short cycling time. It exhibits good hydrolytic stability, excellent abrasion resistance, toughness, good heat, oil, fuel, and solvent resistance. It has excellent damping characteristics and outstanding resistance to tear propagation. Elastollan® S85AN is rated UL-94 HB in vertical flame test for wall thickness of 0.95 mm. Elastollan® S85AN is supplied uncolored in diced form. |
General Information | |
---|---|
Features |
|
Appearance |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.22 | g/cm³ | ASTM D792 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A) | 84 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Modulus (Injection Molded) | 19.3 | MPa | ASTM D412 |
Flexural Modulus (Injection Molded) | 24.1 | MPa | ASTM D790 |
Taber Abrasion Resistance | 25.0 | mg | ASTM D1044 |
Abrasion - DIN | 25 | mm³ | DIN 53516 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Softening Point - DMA | 116 | °C | Internal Method |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | ASTM D412 | ||
100% Strain | 8.96 | MPa | |
300% Strain | 19.3 | MPa | |
Tensile Strength | 42.1 | MPa | ASTM D412 |
Tensile Elongation (Break) | 600 | % | ASTM D412 |
Tear Strength 1 | 110 | kN/m | ASTM D624 |
Compression Set | ASTM D395B | ||
23°C, 22 hr | 25 | % | |
70°C, 22 hr | 35 | % |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Glass Transition Temperature | -31.0 | °C | Internal Method |
Vicat Softening Temperature | 110 | °C | ASTM D1525 |
Flammability | Nominal Value | Test Method | |
---|---|---|---|
Flame Rating (0.950 mm) | HB | UL 94 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 100 to 110 | °C | |
Drying Time | 2.0 to 3.0 | hr | |
Suggested Max Moisture | 0.030 | % |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 100 to 110 | °C | |
Drying Time | 2.0 to 3.0 | hr | |
Cylinder Zone 1 Temp. | 160 to 200 | °C | |
Cylinder Zone 3 Temp. | 160 to 200 | °C | |
Cylinder Zone 5 Temp. | 160 to 200 | °C | |
Adapter Temperature | 175 to 200 | °C | |
Die Temperature | 175 to 205 | °C |
Note Message | |
---|---|
1 . | Die C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Maxelast® D6890 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
RTP 2309 A | RTP Company | PUR, Unspecified | RTP |
TAIRILITE AC3610 | Formosa Plastics Corporation | PC | TAIRILITE |
Flontech® FT-1-1L | Guarniflon S.p.A. - Flontech Division | PTFE | Flontech® |
CERTENE™ PHM-35AN | Muehlstein | PP Homopolymer | CERTENE™ |