Category: | PUR-Ether/TDI , Polyurethane (Polyether, TDI) |
Manufacturer: | Anderson Development Company |
Trademark: | Andur |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | e2wFGg_Andur-7501-DP-Curene-442.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Andur 7501-DP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 73 to 77 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers. |
General Information | |
---|---|
Forms |
|
Hardness | Nominal Value | Test Method | |
---|---|---|---|
Durometer Hardness (Shore D) | 75 | ASTM D2240 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 31.7 | MPa | ASTM D412 |
Tensile Strength (Yield) | 44.1 | MPa | ASTM D412 |
Tensile Elongation (Break) | 250 | % | ASTM D412 |
Bayshore Resilience | 58 | % | ASTM D2632 |
Thermoset | Nominal Value | Unit | |
---|---|---|---|
Pot Life | 3.0 - 3.5 | min | |
Demold Time (100°C) | 15 | min | |
Post Cure Time (100°C) | 16 | hr |
Additional Information |
---|
Durometer Hardness, ASTM D2240, Shore D: 73 to 77Die C Tear, ASTM D1004: 780 pliAverage Split Tear, ASTM D1938: 290 pliStoichiometry Curative Level: 95%Mix Temperature: Andur 7501 DP: 180-212°F Curene 442: 230-240°F |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1607 | RTP Company | PAS | RTP |
Evermore PUR SS-1058NHR | Evermore Chemical Industry Co., Ltd. | PUR, Unspecified | Evermore PUR |
Dryflex® WS 25E450 | ELASTO | TPE | Dryflex® |
HIPLEX® HUM 45010 | HIP-PetroHemija | HDPE | HIPLEX® |
Petrothene® NA952000 | LyondellBasell Industries | LDPE | Petrothene® |