Monprene® CE-22968

Category: TPE , Thermoplastic Elastomer
Manufacturer: Teknor Apex Company
Trademark: Monprene®
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: dyWaVQ_Monprene-CE-22968.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Monprene®CE-22968 is a thermoplastic elastomer (TPE) material,. This product is available in the Asia-Pacific region and is processed by extrusion or injection molding.

Typical application areas include:
  • Handle
  • safety equipment
  • packing
  • kitchen utensils
  • engineering/industrial accessories
General Information
Uses
  • Safety equipment
  • Handle
  • Packaging
  • Kitchen utensils
  • Washer
  • Pipe fittings
  • Sporting goods
  • Shell
  • Stationery
  • Consumer goods application field
  • Toothbrush handle
  • Medical/nursing supplies
Appearance
  • Natural color
Forms
  • Particle
Processing Method
  • Extrusion
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.920g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg)3.0g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shaw A 70ASTM D2240
    Shaw A, 5 seconds 68ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress ASTM D412
    100% strain 1.90MPaASTM D412
    300% strain 3.30MPaASTM D412
Tensile Strength (Break)12.0MPaASTM D412
Tensile Elongation (Break)600%ASTM D412
Compression Set ASTM D395B
    -15°C, 22 hr 28%ASTM D395B
    23°C, 22 hr 26%ASTM D395B
    70°C, 22 hr 50%ASTM D395B
    100°C, 22 hr 68%ASTM D395B
    125°C, 22 hr 88%ASTM D395B
InjectionNominal ValueUnit
Rear Temperature 182 - 232°C
Middle Temperature 188 - 238°C
Front Temperature 193 - 243°C
Nozzle Temperature 199 - 249°C
Processing (Melt) Temp 199 - 249°C
Mold Temperature 35.0 - 48.9°C
Injection Pressure 1.38 - 5.52MPa
Injection Rate Fast
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ExtrusionNominal ValueUnit
Cylinder Zone 1 Temp. 182 - 232°C
Cylinder Zone 2 Temp. 188 - 238°C
Cylinder Zone 3 Temp. 193 - 243°C
Cylinder Zone 5 Temp. 199 - 249°C
Die Temperature 199 - 249°C
Extrusion instructions
Screw Speed: 30 to 100 rpm
Resin Grade Manufacturer Category Trademark
RTP ESD A 680 FR RTP Company ABS RTP
Sumikon® EME-9300H Sumitomo Bakelite Co., Ltd. Epoxy Sumikon®
DIAMALOY ABSPC 754M Network Polymers, Inc. PC+ABS DIAMALOY ABSPC
LNP™ THERMOCOMP™ 9X11428J compound SABIC Innovative Plastics PPS LNP™ THERMOCOMP™
Sylvin 5143-88 White 1318 Sylvin Technologies Incorporated PVC, Unspecified Sylvin