| Category: | ABS , Acrylonitrile Butadiene Styrene |
| Manufacturer: | ALBIS PLASTIC GmbH |
| Trademark: | ALTECH® ABS |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | dlScXV_ALTECH-ABS-A-1000-627-UV.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
ALTECH® ABS A 1000/627 UV is an Acrylonitrile Butadiene Styrene (ABS) product. It can be processed by injection molding and is available in Asia Pacific, Europe, or North America. Characteristics include:
|
| General Information | |
|---|---|
| Additive |
|
| Features |
|
| Agency Ratings |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.00 | g/cm³ | ISO 1183 |
| Melt Volume-Flow Rate (MVR) (220°C/10.0 kg) | 20.0 | cm³/10min | ISO 1133 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2350 | MPa | ISO 527-2 |
| Tensile Stress | ISO 527-2 | ||
| Yield | 50.0 | MPa | |
| -- | 45.0 | MPa | |
| Tensile Strain | ISO 527-2 | ||
| Yield | 3.0 | % | |
| Break | 7.0 | % | |
| Flexural Modulus | 2380 | MPa | ISO 178 |
| Flexural Stress | ISO 178 | ||
| -- | 75.0 | MPa | |
| 3.5% Strain | 72.0 | MPa |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | ||
| -- | 12 | kJ/m² | |
| -40°C | 5.0 | kJ/m² | |
| -20°C | 6.0 | kJ/m² | |
| Charpy Unnotched Impact Strength | No Break | ISO 179/1eU |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Vicat Softening Temperature | 105 | °C | ISO 306/B50 |
| Flammability | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Flame Rating | UL 94 | ||
| 0.750 mm | HB | ||
| 1.50 mm | HB | ||
| 3.00 mm | HB | ||
| Glow Wire Flammability Index | IEC 60695-2-12 | ||
| 1.00 mm | 650 | °C | |
| 2.00 mm | 650 | °C | |
| 3.00 mm | 650 | °C |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | |||
| Circulation Dryer | 80.0 | °C | |
| Desiccant Dryer | 80.0 | °C | |
| Drying Time | |||
| Circulation Dryer | 3.0 to 6.0 | hr | |
| Desiccant Dryer | 2.0 to 4.0 | hr | |
| Processing (Melt) Temp | 220 to 260 | °C | |
| Mold Temperature | 50.0 to 80.0 | °C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Maxelast® N8955 | Nantong Polymax Elastomer Technology, Co., Ltd | TPE | Maxelast® |
| RTP 800 GB 25 | RTP Company | Acetal (POM) Copolymer | RTP |
| SABIC® PPcompound 108CSF10 | Saudi Basic Industries Corporation (SABIC) | PP, Unspecified | SABIC® PPcompound |
| Elastollan® Soft 45 A ESD | BASF Polyurethanes GmbH | TPU-Polyester | Elastollan® |
| OTECH PVC OW742-MT - A/V Jacket | OTECH Corporation | PVC, Unspecified | OTECH PVC |