PENTAMID B GV20 H natur

Category: Nylon 6 , Polyamide 6
Manufacturer: PENTAC Polymer GmbH
Trademark: PENTAMID B
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: dkPAhC_PENTAMID-B-GV20-H-natur.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Normal viscosity, heat stabilised polyamide 6, 20% glass fiber reinforced
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 20% filler by weight
Additive
  • heat stabilizer
Features
  • Rigid, good
  • Thermal Stability
  • Excellent appearance
Uses
  • Shell
Agency Ratings
  • EC 1907/2006 (REACH)
Appearance
  • Natural color
Forms
  • Particle
PhysicalDryConditionedUnitTest Method
Density 1.27--g/cm³ISO 1183
Molding Shrinkage ISO 294-4
     Vertical flow direction 0.80--%ISO 294-4
     Flow direction 0.55--%ISO 294-4
Water Absorption ISO 62
     Saturated, 23°C 7.6--%ISO 62
     Equilibrium, 23°C, 50% RH 2.4--%ISO 62
Viscosity Number 145--cm³/gISO 307
HardnessDryConditionedUnitTest Method
Ball Indentation Hardness (H 961/30)195--MPaISO 2039-1
MechanicalDryConditionedUnitTest Method
Tensile Modulus 70004600MPaISO 527-2/1
Tensile Stress (Break)14085.0MPaISO 527-2
Tensile Strain (Break)4.09.0%ISO 527-2
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)1013kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)6585kJ/m²ISO 179/1eU
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature
     0.45 MPa, not annealed 215--°CISO 75-2/B
     1.8 MPa, not annealed 200--°CISO 75-2/A
Melting Temperature (DSC) 222--°CISO 3146
ElectricalDryConditionedUnitTest Method
Dielectric Strength (1.00 mm)34--kV/mmIEC 60243-1
Relative Permittivity (1 MHz)3.80--IEC 60250
Comparative Tracking Index 500--VIEC 60112
FlammabilityDryConditionedUnitTest Method
Flame Rating (3.20 mm)HB--UL 94
Additional Information
干燥 ISO Description: PA6, MHR, 14-070 N, GF20The value listed as Melting Point, ISO 3146, was tested in accordance with ISO 11357.
调节后的 ISO Description: PA6, MHR, 14-070 N, GF20
InjectionDryUnit
Drying Temperature 80.0°C
Drying Time 3.0hr
Suggested Max Moisture 0.090%
Suggested Max Regrind 20%
Rear Temperature 255 - 280°C
Middle Temperature 275 - 285°C
Front Temperature 275 - 280°C
Processing (Melt) Temp 280°C
Mold Temperature 80.0°C
Injection Pressure 65.0MPa
Holding Pressure 39.0MPa
Screw L/D Ratio 20.0:1.0
Screw Compression Ratio 2.2:1.0 to 2.8:1.0
Resin Grade Manufacturer Category Trademark
Synthos EPS® 0513F/CZ Synthos S.A. PS (EPS) Synthos EPS®
ACCUTECH™ CP0437T10L ACLO Compounders Inc. PP Copolymer ACCUTECH™
ALTECH® PP-B A 4920/500 MR20 ALBIS PLASTIC GmbH PP Copolymer ALTECH® PP-B
Ferro PP TPP40AF58UL ALMOND Ferro Corporation PP Homopolymer Ferro PP
Geon™ Vinyl Flexible R4294W PolyOne Corporation PVC, Flexible Geon™ Vinyl Flexible