Category: | PP Copolymer , Polypropylene Copolymer |
Manufacturer: | Polykemi AB |
Trademark: | POLYpropen |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | dbYeTT_POLYpropen-PPC-15000.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
PP copolymer |
General Information |
---|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.910 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 15 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.5 to 1.8 | % | |
Flow | 1.5 to 1.8 | % |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 28.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 6.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 1300 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 3.0 | kJ/m² | |
23°C | 7.0 | kJ/m² | |
Charpy Unnotched Impact Strength (23°C) | No Break | ISO 179 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1 | |||
0.45 MPa, Unannealed | 90.0 | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 53.0 | °C | ISO 75-2/A |
Vicat Softening Temperature | |||
-- | 151 | °C | ISO 306/A50 |
-- | 68.0 | °C | ISO 306/B50 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating (1.60 mm) | HB | UL 94 | |
Glow Wire Ignition Temperature (2.00 mm) | 650 | °C | IEC 60695-2-13 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Tecnoprene® AK7HCT NAT001 | SO.F.TER. SPA | PP Homopolymer | Tecnoprene® |
SUPREME Specialty PS SP255 | Supreme Petrochem Ltd. | PS (Specialty) | SUPREME Specialty PS |
Trexprene® A88BW | Mitsubishi Chemical Performance Polymers, Inc. | TPV | Trexprene® |
Bormed™ HD800CF | Borealis AG | PP Homopolymer | Bormed™ |
RTP 299 F X 125585 H | RTP Company | Nylon 12 | RTP |