| Category: | Silicone Rubber, HTV , Silicone Rubber, HTV |
| Manufacturer: | Shin-Etsu Silicones of America |
| Trademark: | Shin-Etsu Elastomer |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | daEtNp_Shin-Etsu-Elastomer-SV-16000U.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
SV-16000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering.
Typical Applications
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Specific Gravity | 1.19 | g/cm³ |
| Hardness | Nominal Value | Unit | |
|---|---|---|---|
| Durometer Hardness | 59 |
| Elastomers | Nominal Value | Unit | |
|---|---|---|---|
| Tensile Strength | 10.1 | MPa | |
| Tensile Elongation (Break) | 380 | % | |
| Tear Strength 1 | 21.5 | kN/m | |
| Compression Set (177°C, 22 hr) | 14 | % |
| Thermoset | Nominal Value | Unit | |
|---|---|---|---|
| Post Cure Time (200°C) | 4.0 | hr |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Cure Agent | DCBP | ||
| Press / Post Cure: Press |
| Uncured Properties | Nominal Value | Unit | |
|---|---|---|---|
| Curing Time | 0.17 | hr |
| Note Message | |
|---|---|
| 1 . | B mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Ultramid® B36 | BASF Corporation | Nylon 6 | Ultramid® |
| Axiall PVC 59996J | Axiall Corporation | PVC, Flexible | Axiall PVC |
| EverGlide® MB5550P-WC | Polymer Dynamix | XLPE | EverGlide® |
| LightSpan® LS-3443 | NuSil Technology | Silicone | LightSpan® |
| PENTAMID AB MA30T H grau 7035/1 | PENTAC Polymer GmbH | Nylon 66/6 | PENTAMID AB |