| Category: | Nylon 66 , Polyamide 66 |
| Manufacturer: | Wellman Engineering Resins |
| Trademark: | EcoLon® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | dP2g5u_EcoLon-MR1660-BK1.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
EcoLon® MR1660-BK1 is a Polyamide 66 (Nylon 66) material filled with 40% mineral. It is available in Asia Pacific, Europe, Latin America, or North America for injection molding. Primary attribute of EcoLon® MR1660-BK1: Eco-Friendly/Green. Typical application of EcoLon® MR1660-BK1: Automotive |
| General Information | |
|---|---|
| Filler / Reinforcement |
|
| Recycled Content |
|
| Appearance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.49 | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | ||
| Across Flow : 23°C | 1.0 to 1.4 | % | |
| Flow : 23°C | 0.70 to 1.1 | % |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (Yield, 23°C) | 70.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield, 23°C) | 3.0 | % | ISO 527-2 |
| Flexural Modulus (23°C) | 7200 | MPa | ISO 178 |
| Flexural Stress (23°C) | 120 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength (23°C) | 3.5 | kJ/m² | ISO 180 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature (1.8 MPa, Unannealed) | 170 | °C | ISO 75-2/A |
| Melting Temperature | 260 | °C | ISO 3146 |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| TEDUR® L 9510-1 | ALBIS PLASTIC GmbH | PPS | TEDUR® |
| Toler PP PP3832 | Toler Chemical, Inc | PP Impact Copolymer | Toler PP |
| DJSilicone NE-7280 | DONGJUE SILICONE (NANJING) CO., LTD | Silicone | DJSilicone |
| ICORENE® 3560 AMBR | A. Schulman Europe | LLDPE | ICORENE® |
| Axiall PVC 4100-50 | Axiall Corporation | PVC, Flexible | Axiall PVC |