| Category: | PPE+PS , Polyphenylene Ether + PS |
| Manufacturer: | SABIC Innovative Plastics Europe |
| Trademark: | NORYL™ |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | dFIiKT_NORYL-6390H-resin.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
PPO |
| General Information | |
|---|---|
| RoHS Compliance |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 1.07 | g/cm³ | ISO 1183 |
| Melt Volume-Flow Rate (MVR) | ISO 1133 | ||
| 280°C/10.0 kg | 4.00 | cm³/10min | |
| 280°C/21.6 kg | 10.0 | cm³/10min |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 2500 | MPa | ISO 527-2/1 |
| Tensile Stress | ISO 527-2/50 | ||
| Yield | 81.0 | MPa | |
| Break | 77.0 | MPa | |
| Tensile Strain | ISO 527-2/50 | ||
| Yield | 5.0 | % | |
| Break | 7.0 | % | |
| Flexural Modulus 1 | 2600 | MPa | ISO 178 |
| Flexural Stress | 115 | MPa | ISO 178 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact Strength 2 | ISO 180/1A | ||
| -30°C | 5.0 | kJ/m² | |
| 23°C | 5.0 | kJ/m² |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Heat Deflection Temperature 3(1.8 MPa, Unannealed, 64.0 mm Span) | 165 | °C | ISO 75-2/Af |
| Glass Transition Temperature | 198 | °C | DSC |
| Vicat Softening Temperature | 191 | °C | ISO 306/B120 |
| Note Message | |
|---|---|
| 1 . | 2.0 mm/min |
| 2 . | 80*10*4 |
| 3 . | 80*10*4 mm |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| WELLAMID Nylon 6000 HWV0CP | CP-Polymer-Technik GmbH & Co. KG | Nylon 6 | WELLAMID Nylon |
| 3M™ Dyneon™ PTFE Compound TF 7921 | 3M Advanced Materials Division | PTFE | 3M™ Dyneon™ PTFE Compound |
| AKROMID® A3 S1 black 9500 (1114) | AKRO-PLASTIC GmbH | Nylon 66 | AKROMID® |
| AKROMID® B3 GF 60 1 natural (2468) | AKRO-PLASTIC GmbH | Nylon 6 | AKROMID® |
| Sumiliteresin® PR-53056 | SBHPP | Phenolic | Sumiliteresin® |