| Category: | Nylon 66 , NYLON RESIN |
| Manufacturer: | DuPont Performance Polymers |
| Trademark: | Zytel® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | dBz66P_Zytel-FG133F1-NC010.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Unreinforced Polyamide 66 with Developed for Food Contact Applications |
| General Information | |
|---|---|
| Additive |
|
| Forms |
|
| Processing Method |
|
| Physical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Density | 1.14 | -- | g/cm³ | ISO 1183 |
| Molding Shrinkage | ISO 294-4 | |||
| Across Flow | 1.0 | -- | % | |
| Flow | 0.70 | -- | % |
| Mechanical | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Tensile Modulus | 3400 | 1940 | MPa | ISO 527-2 |
| Tensile Stress (Yield) | 93.0 | 65.0 | MPa | ISO 527-2 |
| Tensile Strain (Yield) | 4.7 | 19 | % | ISO 527-2 |
| Nominal Tensile Strain at Break | 14 | 40 | % | ISO 527-2 |
| Impact | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Charpy Notched Impact Strength (23°C) | 4.0 | 10 | kJ/m² | ISO 179/1eA |
| Thermal | Dry | Conditioned | Unit | Test Method |
|---|---|---|---|---|
| Heat Deflection Temperature | ||||
| 0.45 MPa, Unannealed | 221 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 78.0 | -- | °C | ISO 75-2/A |
| Melting Temperature 1 | 262 | -- | °C | ISO 11357-3 |
| Note Message | |
|---|---|
| 1 . | 10°C/min |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Rotec® ABS E/S 200 | ROMIRA GmbH | ABS | Rotec® ABS |
| Mylar® A (200 guage) | DuPont Teijin Films U.S. | PET | Mylar® |
| Borclear™ RC737MO | Borealis AG | PP Random Copolymer | Borclear™ |
| INNOPOL® PP CS 1-5830 MA | Inno-Comp Ltd. | PP Homopolymer | INNOPOL® PP |
| Sylvin 5219-92 Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |