RTP ESD C 101

Category: PP, Unspecified , Polypropylene
Manufacturer: RTP Company
Trademark: RTP
Fillers: -
Ports: Qinzhou, Shekou, Shanghai, Ningbo
Delivery Terms FOB, CIF, DAP, DAT, DDP
PDF: d9YD6w_RTP-ESD-C-101.pdf
PRICE: ​Order Products​ email   sales@su-jiao.com
Wechat: WECHAT
Message
Glass Fiber - ESD Protection - Electrically Conductive
General Information
Filler / Reinforcement
  • Glass Fiber, 10% Filler by Weight
Features
  • Electrically Conductive
  • ESD Protection
RoHS Compliance
  • Contact Manufacturer
Processing Method
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 1.06g/cm³ASTM D792
Molding Shrinkage - Flow (3.20 mm)0.40 to 0.60%ASTM D955
MechanicalNominal ValueUnitTest Method
Tensile Modulus 2340MPaASTM D638
Tensile Strength 28.3MPaASTM D638
Tensile Elongation (Yield)6.0 to 9.0%ASTM D638
Flexural Modulus 1860MPaASTM D790
Flexural Strength 41.4MPaASTM D790
ImpactNominal ValueUnitTest Method
Notched Izod Impact (3.20 mm)190J/mASTM D256
Unnotched Izod Impact (3.20 mm)430J/mASTM D4812
ElectricalNominal ValueUnitTest Method
Surface Resistivity
    -- < 1.0E+6ohmsASTM D257
    -- < 1.0E+5ohmsESD STM11.11
Volume Resistivity < 1.0E+3ohms·cmASTM D257
Static Decay 1< 2.0secFTMS 101C 4046.1
Additional InformationNominal ValueUnit
Primary Additive 10%
InjectionNominal ValueUnit
Drying Temperature 79.4°C
Drying Time 2.0hr
Processing (Melt) Temp 191 to 232°C
Mold Temperature 32.2 to 65.6°C
Injection Pressure 68.9 to 103MPa
Note Message
1 .MIL-PRF-81705D, 5kV to 50 V, 12% RH
Resin Grade Manufacturer Category Trademark
Selvol™ MH-82 Sekisui Chemical Company, Ltd. PVOH Selvol™
4MID® 9A22140 4Plas Nylon 66 4MID®
KRYSTALFLEX™ PE499 Huntsman Corporation PUR-Eth,aliphat KRYSTALFLEX™
OmniCarb™ PC08FR GF40 OMNI Plastics, LLC PC OmniCarb™
Sarlink® TPE ML-1190N NAT (PRELIMINARY DATA) Teknor Apex Company TPE Sarlink® TPE