Category: | Nylon 11 , Polyamide 11 |
Manufacturer: | Arkema |
Trademark: | Rilsan® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | cVkuDY_Rilsan-BMN-P20-D.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Rilsan® BMN P20 D is a Polyamide 11 (Nylon 11) product. It can be processed by injection molding and is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America. Characteristics include:
|
General Information | |
---|---|
Additive |
|
Features |
|
Forms |
|
Processing Method |
|
Multi-Point Data |
|
Physical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Density | 1040 | 1040 | kg/m³ | ISO 1183 1 |
Melt volume-flow rate (235°C/2.16 kg) | 18.5 | -- | cm³/10min | ISO 1133 2 |
Water Absorption (Saturation) | 1.8 | -- | % | ISO 62 3 |
Mechanical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Tensile modulus | 540 | 480 | MPa | ISO 527-2 4 |
Tensile Stress (Yield) | 31.0 | 29.0 | MPa | ISO 527-2 5 |
Tensile Strain (Yield) | 35 | 30 | % | ISO 527-2 6 |
Nominal strain at break | > 50 | > 50 | % | ISO 527-2 7 |
Impact | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Charpy notched impact strength | ISO 179/1eA 8 | |||
-30°C | 5.00 | 7.00 | kJ/m² | |
23°C | 19.0 | 37.0 | kJ/m² | |
Charpy impact strength | ISO 179/1eU 9 | |||
-30°C | No Break | No Break | ||
23°C | No Break | No Break |
Thermal | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Deflection Temperature Under Load | ISO 75-2 10 | |||
0.45 MPa | 135 | -- | °C | |
1.8 MPa | 47.0 | -- | °C | |
Vicat Softening Temperature (50°C/h, B (50N)) | 145 | -- | °C | ISO 306 11 |
Melting Temperature 12 | 187 | -- | °C | ISO 11357-3 13 |
CLTE - Flow | 1.0E-4 | -- | cm/cm/°C | ISO 11359-2 14 |
Electrical | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Surface resistivity | -- | 2.0E+12 | ohms | IEC 60093 15 |
Volume resistivity | -- | 1.0E+10 | ohms·m | IEC 60093 16 |
Electric strength | -- | 26 | kV/mm | IEC 60243-1 17 |
Relative Permittivity | IEC 60250 18 | |||
100 Hz | 7.00 | -- | ||
1 MHz | 3.00 | -- | ||
Dissipation Factor | IEC 60250 19 | |||
100 Hz | 0.19 | -- | ||
1 MHz | 0.061 | -- | ||
Comparative tracking index | -- | 600 | IEC 60112 20 |
Flammability | Dry | Conditioned | Unit | Test Method |
---|---|---|---|---|
Burning Behav. at 1.6mm nom. thickn. (1.60 mm) | HB | -- | ISO 1210 21 | |
Burning Behav. at thickness h (3.20 mm) | HB | -- | ISO 1210 22 | |
Oxygen index | 22 | -- | % | ISO 4589-2 23 |
Note Message | |
---|---|
1 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
2 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
3 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
4 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
5 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
6 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
7 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
8 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
9 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
10 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
11 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
12 . | 10 °C/min |
13 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
14 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
15 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
16 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
17 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
18 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
19 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
20 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
21 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
22 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
23 . | Tested in accordance with ISO 10350. 23°C/50%r.h. unless otherwise noted. |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
PROTEQ™ X30S750 | Qenos Pty Ltd | PP, Unspecified | PROTEQ™ |
Sinvicomp SIM5520 | Teknor Apex Asia Pacific PTE. LTD. | PVC, Flexible | Sinvicomp |
MOSTEN EH 501 | UNIPETROL RPA | PP Copolymer | MOSTEN |
Elastron® V V100.A73.B | Elastron USA, Inc. | TPV | Elastron® V |
Sumiliteresin® PR-50385 | SBHPP | Phenolic | Sumiliteresin® |