| Category: | TPU, Unspecified , Thermoplastic Polyurethane Elastomer |
| Manufacturer: | RTP Company |
| Trademark: | RTP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | bcZl1K_RTP-1200-75D.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Warning: The status of this material is 'Commercial: Limited Issue' The data for this material has not been recently verified. Please contact RTP Company for current information prior to specifying this grade. |
| General Information | |
|---|---|
| RoHS Compliance |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.21 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.18 mm, Injection Molded) | 1.0 | % | ASTM D955 |
| Water Absorption (23°C, 24 hr) | 0.30 | % | ASTM D570 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore D) | 75 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Strength (Break) | 40.0 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 360 | % | ASTM D412 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 160 to 210 | °C | |
| Middle Temperature | 160 to 210 | °C | |
| Front Temperature | 160 to 210 | °C | |
| Mold Temperature | 38.0 to 60.0 | °C | |
| Injection Pressure | 69.0 to 103 | MPa |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Salflex 255 | Salflex Polymers Ltd. | TPO (POE) | Salflex |
| TRIREX® 3022PJ(01) | Samyang Corporation | PC | TRIREX® |
| Mylar® A (92 guage) | DuPont Teijin Films U.S. | PET | Mylar® |
| Dryflex® 602850S | ELASTO | SEBS | Dryflex® |
| Monprene® CP-32054G CLR | Teknor Apex Company | TPE | Monprene® |