Sarlink TPE OM series are high performance specialty thermoplastic elastomers designed for automotive applications requiring excellent bondability to engineered resin substrates. Sarlink TPE OM-1150N is a medium hardness, medium density, opaque grade with good UV resistance that exhibits excellent adhesion to ABS, PC, and PC/ABS.
General Information
Features
  • Without Fillers
  • Good UV resistance
  • Workability, good
  • Adhesiveness
  • Good adhesion
  • Medium liquidity
  • Good chemical resistance
  • Medium density
  • Medium hardness
Uses
  • overmolding
  • Automotive Electronics
  • Application in Automobile Field
  • Car interior parts
  • Soft touch application
RoHS Compliance
  • RoHS compliance
Appearance
  • Opacity
  • Natural color
Forms
  • Particle
Processing Method
  • Injection molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 0.998g/cm³ASTM D792
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg)15g/10 minASTM D1238
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240
    Shore A, 1 second, injection molding 145ASTM D2240
    Shore A, 5 seconds, injection molding 255ASTM D2240
ElastomersNominal ValueUnitTest Method
Tensile Stress 3ASTM D412
    Transverse flow : 100% strain 1.48MPaASTM D412
    Flow : 100% strain 1.65MPaASTM D412
    Transverse flow : 300% strain 2.90MPaASTM D412
    Flow : 300% strain 3.27MPaASTM D412
Tensile Strength 4ASTM D412
    Transverse flow : Fracture 5.67MPaASTM D412
    Flow : Fracture 5.87MPaASTM D412
Tensile Elongation 5ASTM D412
    Transverse flow : Fracture 550%ASTM D412
    Flow : Fracture 540%ASTM D412
Compression Set 6ASTM D395B
    23°C, 22 hr 42%ASTM D395B
    70°C, 22 hr 91%ASTM D395B
Additional InformationNominal ValueUnit
Adhesion Strength - Cohesive Failure 51N
Adhesion to ABS
Adhesion to PC
Adhesion to PC/ABS
Legal statement
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
InjectionNominal ValueUnit
Drying Temperature 60°C
Drying Time 2.0 - 4.0hr
Rear Temperature 138 - 188°C
Middle Temperature 154 - 199°C
Front Temperature 154 - 216°C
Nozzle Temperature 154 - 221°C
Processing (Melt) Temp 166 - 221°C
Mold Temperature 10 - 32°C
Injection Pressure 1.38 - 5.52MPa
Injection Rate Moderate-Fast
Back Pressure 0.172 - 0.862MPa
Screw Speed 50 - 100rpm
Cushion 3.81 - 25.4mm
Injection instructions
Moisture can degrade the material. Drying is suggested. This can be accomplished by placing the material in a desiccant dryer for 2 to 4 hours at140°F.
Note Message
1 .Aging 0 hr at 23°C
2 .Aging 48 hr at 23°C
3 .C mold, 510mm/min
4 .C mold, 510mm/min
5 .C mold, 510mm/min
6 .Type 1
Resin Grade Manufacturer Category Trademark
Telcar® TL-1140E Teknor Apex Company TPE Telcar®
Tarflen® SM-S15G2 Grupa Azoty S.A. PTFE Tarflen®
ALTECH® PC A 1000/326 UV ALBIS PLASTIC GmbH PC ALTECH® PC
Aristech Quarite Plus® Aristech Acrylics LLC Acrylic, Unspecified Aristech
POLYLAC® PA-757GJ08 CHI MEI CORPORATION ABS POLYLAC®