| Category: | PC+ABS , Polycarbonate + ABS |
| Manufacturer: | RTP Company |
| Trademark: | RTP |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | bEcEY5_RTP-2599-X-125099.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| EMI/RFI Shielding - Electrically Conductive |
| General Information | |
|---|---|
| Features |
|
| RoHS Compliance |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 1.36 | g/cm³ | ASTM D792 |
| Molding Shrinkage - Flow (3.20 mm) | 0.25 | % | ASTM D955 |
| Moisture Content | 0.020 | % |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Static Decay | sec | FTMS 101C 4046.1 |
| Mechanical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Modulus | 5860 | MPa | ASTM D638 |
| Tensile Strength | 82.7 | MPa | ASTM D638 |
| Tensile Elongation (Yield) | 1.5 - 2.5 | % | ASTM D638 |
| Flexural Modulus | 5860 | MPa | ASTM D790 |
| Flexural Strength | 130 | MPa | ASTM D790 |
| Impact | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Notched Izod Impact (3.20 mm) | 48 | J/m | ASTM D256 |
| Unnotched Izod Impact (3.20 mm) | 330 | J/m | ASTM D4812 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Deflection Temperature Under Load (1.8 MPa, Unannealed) | 118 | °C | ASTM D648 |
| Electrical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Surface Resistivity | |||
| -- | < 1.0E+4 | ohms | ASTM D257 |
| -- | < 1.0E+3 | ohms | ESD STM11.11 |
| Volume Resistivity | < 1.0 | ohms·cm | ASTM D257 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Drying Temperature | 93.3 | °C | |
| Drying Time | 4.0 | hr | |
| Dew Point | -28.9 | °C | |
| Processing (Melt) Temp | 252 - 274 | °C | |
| Mold Temperature | 43.3 - 60.0 | °C | |
| Injection Pressure | 68.9 - 103 | MPa |
| Injection instructions |
|---|
| Use a reverse barrel profile. Remove hopper magnets. Allow 4 - 5 shots to properly disperse the conductive fibers. The surface finish should have a silver streaking appearance, not clumps.Remove hopper magnets.Desiccant Type Dryer Required. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| RTP 280.8D | RTP Company | Nylon 612 | RTP |
| TRANSMARE® 35HNF50-0.001 | Transmare Compounding B.V. | PP Homopolymer | TRANSMARE® |
| Diaterm® A27 GF20 | DTR S.r.l. (Develop Thermoplastic Resins) | Nylon 6 | Diaterm® |
| LNP™ LUBRILOY™ RF203AXH compound | SABIC Innovative Plastics | Nylon 66 | LNP™ LUBRILOY™ |
| Sylvin 6235-80UV Grey 9591 | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |