Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | ExxonMobil Chemical |
Trademark: | Santoprene™ |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | apXU81_Santoprene-8221-60.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
It is a soft, colorable, UV-resistant thermoplastic vulcanized elastomer (TPV) in the thermoplastic elastomer (TPE) series. This material has good physical properties and chemical resistance at the same time, and is suitable for a wide range of fields. This brand of Shanduping TPV is a shear rate dependent product that can be processed on conventional thermoplastic injection molding or blow molding equipment. This is a polyolefin-based material that can be recycled in the production process. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
RoHS Compliance |
|
UL File Number |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | |||
-- | 0.948 | g/cm³ | ASTM D792 |
-- | 0.950 | g/cm³ | ISO 1183 |
Outdoor Suitability | f1 | UL 746C |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shaw A, 15 seconds, 23°C, 2.00mm) | 64 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress - Across Flow (100% Strain, 23°C) | 2.20 | MPa | ASTM D412, ISO 37 |
Tensile Strength - Across Flow (Break, 23°C) | 5.70 | MPa | ASTM D412, ISO 37 |
Tensile Elongation - Across Flow (Break, 23°C) | 470 | % | ASTM D412, ISO 37 |
Compression Set | |||
70°C, 22 hr 1 | 32 | % | ASTM D395B |
125°C, 70 hr 2 | 60 | % | ASTM D395B |
70°C, 22 hr 3 | 32 | % | ISO 815 |
125°C, 70 hr 4 | 60 | % | ISO 815 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -63.0 | °C | ASTM D746, ISO 812 |
RTI Elec | 100 | °C | UL 746 |
RTI | 85.0 | °C | UL 746 |
Electrical | Nominal Value | Unit | Test Method |
---|---|---|---|
Dielectric Strength (23°C, 2.00 mm) | 31 | kV/mm | ASTM D149 |
Dielectric Constant (23°C, 2.01 mm) | 2.30 | ASTM D150, IEC 60250 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Flame Rating | UL 94 | ||
1.10 mm | HB | UL 94 | |
3.00 mm | HB | UL 94 |
Additional Information |
---|
如果适用,这是基于扇形浇口注塑成型的平板测试结果。拉伸强度、伸长率和拉伸应力沿垂直流动方向测定 - ISO 1 型,ASTM die C。25% 形变时的永久压缩变形。从埃克森美孚欧洲分支机构直接购买的所有产品都符合 REACH 法规。 对于埃克森 美孚未进口至欧洲的产品,用户应自行评估其是否满足 REACH 法规。 |
Legal statement |
---|
未经埃克森美孚化工书面允许,这种产品包括其产品名称,不得在任何医疗应用领域予以使用或有关详细的产品监管信息,请联系客户服务。 |
Injection | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 82.2 | °C | |
Drying Time | 3.0 | hr | |
Suggested Max Moisture | 0.080 | % | |
Suggested Max Regrind | 20 | % | |
Rear Temperature | 177 - 191 | °C | |
Middle Temperature | 179 - 193 | °C | |
Front Temperature | 185 - 199 | °C | |
Nozzle Temperature | 185 - 210 | °C | |
Processing (Melt) Temp | 143 - 216 | °C | |
Mold Temperature | 23.9 - 51.7 | °C | |
Injection Rate | Fast | ||
Back Pressure | 0.345 - 0.689 | MPa | |
Screw Speed | 100 - 200 | rpm | |
Clamp Tonnage | 4.1 - 6.9 | kN/cm² | |
Cushion | 3.18 - 6.35 | mm | |
Screw L/D Ratio | 16.0:1.0 to 20.0:1.0 | ||
Screw Compression Ratio | 2.0:1.0 to 2.5:1.0 | ||
Vent Depth | 0.025 | mm |
Injection instructions |
---|
Santoprene TPV与乙缩醛和PVC不相容。更多关于加工和模具设计的信息,请查阅我们的《注射成型指南》。 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Melt Temperature | 179 - 216 | °C | |
Die Temperature | 177 - 216 | °C |
Note Message | |
---|---|
1 . | Type 1 |
2 . | Type 1 |
3 . | Type a |
4 . | Type a |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Prime Flexible 7049 CLR | Prime PVC® | PVC, Flexible | Prime Flexible |
Sylvin 8235-90FU Natural | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
TUFNYL® RXXIC GREY | SRF Ltd. | Nylon 66 | TUFNYL® |
ASTALAC™ ASA 314 | Marplex Australia Pty. Ltd. | ASA | ASTALAC™ |
Axiall PVC 9275 J | Axiall Corporation | PVC, Rigid | Axiall PVC |