TECHNYL® C 218 V15 Black is a polyamide 6, heat stabilized, reinforced with 15% of glass fiber, for injection moulding. The product offers an excellent combination between thermal and mechanical properties.
General Information
Filler / Reinforcement
  • Glass fiber reinforced material, 15% filler by weight
Additive
  • heat stabilizer
Features
  • Heat Stabilized - Inorganic
  • Good liquidity
  • Good demoulding performance
Uses
  • Connector
Agency Ratings
  • EC 1907/2006 (REACH)
RoHS Compliance
  • RoHS compliance
Appearance
  • Black
Forms
  • Particle
Processing Method
  • Injection molding
Resin ID (ISO 1043)
  • PA6-GF15
PhysicalDryConditionedUnitTest Method
Density 1.23--g/cm³ISO 1183/A
Water Absorption ISO 62
     23°C, 24 hr 1.2--%ISO 62
     Equilibrium, 23°C, 50% RH 2.6--%ISO 62
MechanicalDryConditionedUnitTest Method
Tensile Modulus (23°C)61002900MPaISO 527-2/1A
Tensile Stress (Break, 23°C)12070.0MPaISO 527-2/1A
Tensile Strain (Break, 23°C)3.56.5%ISO 527-2
Flexural Modulus (23°C)60002800MPaISO 178
Flexural Stress (23°C)200--MPaISO 178
ImpactDryConditionedUnitTest Method
Charpy Notched Impact Strength (23°C)5.516kJ/m²ISO 179/1eA
Charpy Unnotched Impact Strength (23°C)4055kJ/m²ISO 179/1eU
Notched Izod Impact (23°C)5.014kJ/m²ISO 180
ThermalDryConditionedUnitTest Method
Heat Deflection Temperature (1.8 MPa, Unannealed)180--°CISO 75-2/Af
Melting Temperature 222--°CISO 11357-3
ElectricalDryConditionedUnitTest Method
Surface Resistivity 1.0E+141.0E+12ohmsIEC 60093
Volume Resistivity 1.0E+151.0E+13ohms·cmIEC 60093
Dielectric Strength (2.00 mm)--22kV/mmIEC 60243-1
Dissipation Factor 0.0200.090IEC 60250
Comparative Tracking Index (Solution A)550475VIEC 60112
FlammabilityDryConditionedUnitTest Method
Flame Rating UL 94
     0.8 mm HB--UL 94
     1.6 mm HB--UL 94
Glow Wire Flammability Index (1.6 mm)650--°CIEC 60695-2-12
InjectionDryUnit
Drying Temperature 80°C
Suggested Max Moisture 0.20%
Rear Temperature 230 - 235°C
Middle Temperature 235 - 240°C
Front Temperature 240 - 250°C
Mold Temperature 60 - 90°C
Injection instructions
The material is supplied in airtight bags, ready for use. In case that the virgin material has absorbed moisture, it must be dried with a dehumidified air drying equipment, dew point mini -20°C. Recommended time 2-4hInjection Advice: For reinforced polyamide, Solvay recommends the use of steel with a high content of Carbon and purified for polishing to avoid or limit the abrasion. For example: X38CrMoV5-1 (EN Norm) - 1.2367 /1.2343 (DIN Norm) or X160CrMoV12 (EN Norm) - 1.2601 /1.2379 (DIN Norm). For Mould Temperature, in the case of parts where the surface roughness is required we can recommend a temperature of 90°C to 120°C with an optimum at 105°C. The processing parameters like processing temperatures are a recommendation and can be adjusted in function of injection machine size, part geometry / design
Resin Grade Manufacturer Category Trademark
VESTAMID® Care ME55-B Evonik Industries AG PEBA-Ether VESTAMID® Care
Niche PPCG20BK Niche Polymer, LLC PP Copolymer Niche
Cheng Yu FV30G25 Cheng Yu Plastic Company Limited Acetal (POM) Homopolymer Cheng Yu
Diamond ABS 4012B Network Polymers, Inc. ABS Diamond ABS
Sylvin 6177-80 Orange 597 Sylvin Technologies Incorporated PVC, Unspecified Sylvin