Elastocon® 2865ST is a translucent thermoplastic elastomer compound formulated for applications that require super tough rubber-like properties, high resilience, and high tear strength. Elastocon® 2865ST is well suited for consumer goods and industrial applications requiring U.V. stability. Elastocon 2865ST can be overmolded onto polypropylene. Elastocon® 2865ST is supplied as ready to use pellets in 50 lb. quantities. |
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Appearance |
|
| Forms |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Specific Gravity | 0.920 | g/cm³ | ASTM D792 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A) | 65 | ASTM D2240 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (100% Strain) | 2.40 | MPa | ASTM D412 |
| Tensile Strength | 11.9 | MPa | ASTM D412 |
| Tensile Elongation (Break) | 540 | % | ASTM D412 |
| Tear Strength | 32.2 | kN/m | ASTM D624 |
| Injection | Nominal Value | Unit | |
|---|---|---|---|
| Rear Temperature | 177 | °C | |
| Middle Temperature | 188 - 199 | °C | |
| Front Temperature | 193 - 204 | °C | |
| Nozzle Temperature | 199 - 204 | °C | |
| Processing (Melt) Temp | 199 - 204 | °C | |
| Mold Temperature | 38 - 49 | °C | |
| Injection Rate | Slow-Moderate | ||
| Back Pressure | 0.345 - 1.03 | MPa |
| Injection instructions |
|---|
| Elastocon® 2865ST thermoplastic elastomer compound does not require drying. |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Cylinder Zone 1 Temp. | 154 - 160 | °C | |
| Cylinder Zone 2 Temp. | 160 - 171 | °C | |
| Cylinder Zone 3 Temp. | 171 - 177 | °C | |
| Cylinder Zone 4 Temp. | 182 - 188 | °C | |
| Cylinder Zone 5 Temp. | 177 - 182 | °C | |
| Die Temperature | 160 - 171 | °C |
| Extrusion instructions |
|---|
| Screw Speed: 75 to 125 RPM |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Radilon® A CV500 100 NAT | Radici Plastics | Nylon 66 | Radilon® |
| SureSpec HD51-06 | Genesis Polymers | HDPE, HMW | SureSpec |
| NuSil MED-2245 | NuSil Technology | Rubber | NuSil |
| GLS PP YN09 | GLS Polymers Pvt. Ltd. | PP Copolymer | GLS PP |
| Softell TKG 317N C12740 | LyondellBasell Industries | PP Copolymer | Softell |