Category: | TPV , Thermoplastic Vulcanizate |
Manufacturer: | Riken Technos Corp. |
Trademark: | Actymer® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | a21xYB_Actymer-AE-2020S.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Actymer®AE-2020S is a thermoplastic vulcanized rubber (TPV) product,. It is available in North America or Asia Pacific. Features include:
|
General Information | |
---|---|
Features |
|
Forms |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.928 | g/cm³ | ISO 1183 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 15 sec) | 20 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress (100% Strain) | 0.500 | MPa | ISO 37 |
Tensile Stress (Yield) | 4.80 | MPa | ISO 37 |
Tensile Elongation (Break) | 780 | % | ISO 37 |
Tear Strength | 13 | kN/m | ISO 34-1 |
Compression Set | ISO 815 | ||
70°C, 72 hr | 30 | % | ISO 815 |
120°C, 72 hr | 40 | % | ISO 815 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (136°C, 168 hr) | -5.0 | % | ISO 188 |
Change in Tensile Strain at Break in Air (136°C, 168 hr) | -5.0 | % | ISO 188 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Brittleness Temperature | -60.0 | °C | ISO 974 |
Additional Information |
---|
The values listed above are tested in accordance with JIS K test methods.Rebound Resilience: 65% |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
MORETEC™ 00138H | Prime Polymer Co., Ltd. | LLDPE | MORETEC™ |
NEXT SIGNATURE POMC HF-100 | NEXT Specialty Resins, Inc. | Acetal (POM) Copolymer | NEXT SIGNATURE |
ALTECH® PA6 A 3030/109 GB30 | ALBIS PLASTIC GmbH | Nylon 6 | ALTECH® PA6 |
BP RPP 1009 GK | Buckeye Polymers, Inc. | PP, Unspecified | BP |
Lupolen 1800 S | LyondellBasell Industries | LDPE | Lupolen |