IROGRAN A 85 E 4607 is a thermoplastic polyether-polyurethane intended for extrusion and injection moulding applications.

Additional characteristics of the product are excellent mechanical properties and high tear strength.

PERFORMANCE FEATURES
  • Good melt flow
  • High wear resistance
  • High elasticity
  • Oil resistance
  • Low-temperature flexibility

APPLICATIONS
For the production of spiral hoses, tooth belts round cords, casual shoe soles.
General Information
Features
  • Good Flow
  • Good Tear Strength
  • High Elasticity
  • Low Temperature Flexibility
  • Oil Resistant
Uses
  • Belts/Belt Repair
  • Footwear
  • Hose
Forms
  • Pellets
Processing Method
  • Extrusion
  • Injection Molding
PhysicalNominal ValueUnitTest Method
Specific Gravity 11.20g/cm³
Melt Volume-Flow Rate (MVR) (190°C/21.6 kg)35.0cm³/10min
Molding Shrinkage - Flow (Injection Molded)0.60%ASTM D955
HardnessNominal ValueUnitTest Method
Durometer Hardness ASTM D2240, ISO 868
    Shore A, Injection Molded 85
    Shore D, Injection Molded 34
MechanicalNominal ValueUnitTest Method
Abrasion 225mm³ISO 4649
ElastomersNominal ValueUnitTest Method
Tensile Stress 3
    100% Strain 4.90MPaASTM D412
    100% Strain 5.00MPaDIN 53504
    300% Strain 11.0MPaASTM D412
    300% Strain 14.0MPaDIN 53504
Tensile Strength 4
    Break 36.0MPaASTM D412
    Break 45.0MPaDIN 53504
Tensile Elongation 5
    Break 750%ASTM D412
    Break 650%DIN 53504
Tear Strength 6
    -- 99.8kN/mASTM D624
    -- 70kN/mISO 34-1
Compression Set 7ASTM D395, ISO 815
    23°C, 24 hr 25%
    70°C, 24 hr 40%
InjectionNominal ValueUnit
Drying Temperature
    -- 100 to 110°C
    Hot Air Dryer 80.0 to 90.0°C
Drying Time
    -- 3.0hr
    Hot Air Dryer 3.0hr
Dew Point -30.0°C
Rear Temperature 175 to 195°C
Middle Temperature 175 to 195°C
Front Temperature 175 to 195°C
Nozzle Temperature 180 to 200°C
Processing (Melt) Temp 170 to 195°C
Mold Temperature 20.0 to 70.0°C
ExtrusionNominal ValueUnit
Drying Temperature 100 to 110°C
Drying Time 3.0hr
Hopper Temperature 25.0 to 40.0°C
Cylinder Zone 1 Temp. 165 to 190°C
Cylinder Zone 2 Temp. 165 to 190°C
Cylinder Zone 3 Temp. 165 to 190°C
Cylinder Zone 4 Temp. 165 to 190°C
Cylinder Zone 5 Temp. 165 to 190°C
Adapter Temperature 175 to 195°C
Die Temperature 175 to 200°C
Note Message
1 .Injection Molded
2 .Injection Molded
3 .Injection Molded
4 .Injection Molded
5 .Injection Molded
6 .Injection Molded
7 .Injection Molded
Resin Grade Manufacturer Category Trademark
Ravamid® B ST BK45 Ravago Group Nylon 6 Ravamid®
TechnoFin PPC EPDM 4820 TechnoCompound GmbH EPDM TechnoFin
Zytel® 70G30L NC010 DuPont Performance Polymers Nylon 66 Zytel®
NuSil CF2-4721 NuSil Technology Silicone NuSil
Hanwha Total PP RB221 HANWHA TOTAL PETROCHEMICALS Co., Ltd. PP, Unspecified Hanwha Total PP