| Category: | SBC , Styrene Butadiene Block Copolymer |
| Manufacturer: | Riken Technos Corp. |
| Trademark: | Leostomer® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | Zf5q9A_Leostomer-SR2264.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
|
Leostomer®SR2264 is a styrene-butadiene copolymer (SBC) product,. It is available in North America or Asia Pacific. Features include:
|
| General Information | |
|---|---|
| Features |
|
| Forms |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.948 | g/cm³ | ISO 1183 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Durometer Hardness (Shore A, 15 sec) | 60 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress (300% Strain) | 6.50 | MPa | ISO 37 |
| Tensile Stress (Yield) | 12.0 | MPa | ISO 37 |
| Tensile Elongation (Break) | 490 | % | ISO 37 |
| Tear Strength | 25 | kN/m | ISO 34-1 |
| Compression Set | ISO 815 | ||
| -- | 36 | % | ISO 815 |
| 70°C, 22 hr | 27 | % | ISO 815 |
| Aging | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Change in Tensile Strength in Air (120°C, 168 hr) | 0.0 | % | ISO 188 |
| Change in Tensile Strain at Break in Air (120°C, 168 hr) | 0.0 | % | ISO 188 |
| Thermal | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Brittleness Temperature | -60.0 | °C | ISO 974 |
| Additional Information |
|---|
| The values listed above are tested in accordance with JIS K test methods. |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| SCANAMID 6 B12^ | Polykemi AB | Nylon 6 | SCANAMID 6 |
| Ultrason® E 2010 MR SW 10111 | BASF Corporation | PESU | Ultrason® E |
| EchoShield 0512 | DN Plastics | TPO (POE) | EchoShield |
| Elastron® G G400.D40.N | Elastron USA, Inc. | SEBS | Elastron® G |
| Kepital® FS2022 | Korea Engineering Plastics Co., Ltd | Acetal (POM) Copolymer | Kepital® |