| Category: | Silicone Rubber, HTV , Silicone Rubber, HTV |
| Manufacturer: | Shin-Etsu Silicones of America |
| Trademark: | Shin-Etsu Elastomer |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ZSAaNi_Shin-Etsu-Elastomer-SV-14000U.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
SV-14000U is one of a series of easy processing, no post cure silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendering.
Typical Applications
|
| General Information | |
|---|---|
| Features |
|
| Uses |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | |
|---|---|---|---|
| Specific Gravity | 1.09 | g/cm³ |
| Hardness | Nominal Value | Unit | |
|---|---|---|---|
| Durometer Hardness | 40 |
| Elastomers | Nominal Value | Unit | |
|---|---|---|---|
| Tensile Stress (100% Strain) | 1.06 | MPa | |
| Tensile Strength | 5.12 | MPa | |
| Tensile Elongation (Break) | 360 | % | |
| Tear Strength 1 | 10.7 | kN/m | |
| Compression Set (177°C, 22 hr) | 25 | % |
| Additional Information | Nominal Value | Unit | |
|---|---|---|---|
| Cure Agent | DCBP | ||
| Press / Post Cure: Press |
| Uncured Properties | Nominal Value | Unit | |
|---|---|---|---|
| Curing Time | 0.17 | hr |
| Note Message | |
|---|---|
| 1 . | B mould |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| VITAMIDE® BF23BL6571 | Jackdaw Polymers | Nylon 6 | VITAMIDE® |
| Chemlon® 66GF4H | Teknor Apex Company (Chem Polymer) | Nylon 66 | Chemlon® |
| FRIANYL® C3 GF10 TF20 V2XI | Nilit Plastics | Nylon 66/6 | FRIANYL® |
| Durepol® PBT A3 G10 PRTA011 BT319 | Petropol Industry and Trade of Polymers LTDA | PBT | Durepol® PBT |
| OmniCarb™ PC08FR510 | OMNI Plastics, LLC | PC | OmniCarb™ |