Category: | PP+EPDM , Polypropylene + EPDM Rubber |
Manufacturer: | Polykemi AB |
Trademark: | POLYelast |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | ZHEFfU_POLYelast-TPE-R44-T10.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Mineral reinforced |
General Information | |
---|---|
Filler / Reinforcement |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.960 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (230°C/2.16 kg) | 12 | g/10 min | ISO 1133 |
Molding Shrinkage | ISO 294-4 | ||
Across Flow | 1.2 to 1.4 | % | |
Flow | 1.2 to 1.4 | % |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D, 15 sec) | 54 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 19.0 | MPa | ISO 527-2 |
Tensile Strain (Yield) | 8.0 | % | ISO 527-2 |
Flexural Modulus (23°C) | 750 | MPa | ISO 178 |
Flexural Stress | 25.0 | MPa | ISO 178 |
Impact | Nominal Value | Unit | Test Method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179 | ||
-20°C | 15 | kJ/m² | |
23°C | 28 | kJ/m² | |
Charpy Unnotched Impact Strength | ISO 179 | ||
-20°C | No Break | ||
23°C | No Break |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Heat Deflection Temperature 1(0.45 MPa, Unannealed) | 88.0 | °C | ISO 75-2/B |
Vicat Softening Temperature | 132 | °C | ISO 306/A50 |
Note Message | |
---|---|
1 . | 120°C/hr |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
RTP 1300 C TFE 15 | RTP Company | PPS | RTP |
Sumitomo Epoxy E 16521A | Sumitomo Bakelite North America, Inc. | Epoxy | Sumitomo Epoxy |
Sultron® R70 | Asia International Enterprise (Hong Kong) Limited | PPS | Sultron® |
Vi-Chem PVC VDM87-15E/30E-8814 | Vi-Chem Corporation | PVC, Unspecified | Vi-Chem PVC |
Bergadur™ PB400 G10 H UF UV | PolyOne Corporation | PBT | Bergadur™ |