| Category: | TPV , Thermoplastic Vulcanizate |
| Manufacturer: | Taro Plast S.p.A. |
| Trademark: | TAROPRENE® |
| Fillers: | - |
| Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
| Delivery Terms | FOB, CIF, DAP, DAT, DDP |
| PDF: | ZFmkBW_TAROPRENE-2-A55-E1G.pdf |
| PRICE: | Order Products email sales@su-jiao.com |
| Message |
|---|
| Thermoplastic Elastomer Vulcanized. This TPE-V compound combines the typical performance of a vulcanized elastomer with the easy processing of a thermoplastic compound. Taroprene is totally recyclable and it can be produced in standard grades and in tailor-made grades. |
| General Information | |
|---|---|
| Features |
|
| Processing Method |
|
| Physical | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Density | 0.960 | g/cm³ | ISO 1183 |
| Melt Mass-Flow Rate (MFR) (190°C/5.0 kg) | 4.0 | g/10 min | ISO 1133 |
| Hardness | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Shore Hardness (Shore A, 3 sec) | 55 | ISO 868 |
| Elastomers | Nominal Value | Unit | Test Method |
|---|---|---|---|
| Tensile Stress 1 | ASTM D412 | ||
| 100% Strain | 1.75 | MPa | |
| 300% Strain | 2.85 | MPa | |
| Tensile Strength 2(Break) | 4.60 | MPa | ASTM D412 |
| Tensile Elongation 3(Break) | 600 | % | ASTM D412 |
| Tear Strength | 24.8 | kN/m | ASTM D624 |
| Compression Set | ASTM D395B | ||
| 70°C, 22 hr | 34 | % | |
| 100°C, 22 hr | 40 | % |
| Extrusion | Nominal Value | Unit | |
|---|---|---|---|
| Melt Temperature | 150 to 230 | °C |
| Note Message | |
|---|---|
| 1 . | Die C |
| 2 . | Die C |
| 3 . | Die C |
| Resin Grade | Manufacturer | Category | Trademark |
|---|---|---|---|
| Novamid® 2430J | DSM Engineering Plastics | Nylon 66/6 | Novamid® |
| ALCOM® PC 740/4 UV CC1320-08LG | ALBIS PLASTIC GmbH | PC | ALCOM® PC |
| BorSafe™ HE3490-LS-H | Borealis AG | HDPE | BorSafe™ |
| Huafon HF-3385A | Huafon Group Co., Ltd. | TPU-Polyester | Huafon |
| POLYfill PP CQX15015 R3 UV | Polykemi AB | PP, Unspecified | POLYfill |