Category: | Polyolefin, Unspecified , Polyolefin |
Manufacturer: | Crosspolimeri S.p.A. |
Trademark: | FRAGOM |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | Ym5XlG_FRAGOM-PR-444-CD-UV-NERO.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
FRAGOM PR PR/444 CD is a flame retardant polyolefinic compound. FRAGOM PR PR/444 CD UV NERO : FRAGOM PR/444 CD UV BLACK is halogen-free flame-retardant flexible polyolefinic thermoplastic compound with good oxygen index, very easy to process and suitable for UV resistant cable sheathing. Suitable for armored cable sheath. Certify : VDE 0207 HM2/HM4 (K=0,6),CEI 2011 M1,BS 7655 LTS 1-3 |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Specific Gravity | 1.47 | g/cm³ | ASTM D792 |
Melt Mass-Flow Rate (MFR) (190°C/21.6 kg) | 35 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore D) | 47 | ASTM D2240 |
Mechanical | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress | 12.0 | MPa | IEC 60811 |
Tensile Strain (Break) | 180 | % | IEC 60811 |
Aging | Nominal Value | Unit | Test Method |
---|---|---|---|
Change in Tensile Strength in Air (110°C, 168 hr) | -9.0 | % | IEC 60811 |
Change in Tensile Strain at Break in Air (110°C, 168 hr) | -15 | % | IEC 60811 |
Thermal | Nominal Value | Unit | Test Method |
---|---|---|---|
Hot pressing test- 4h at 90°C -Penetration | 40 | % | IEC 60811 |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Halogen Content | 0 | % | IEC 60754-1 |
Toxicity- pH | > 4.50 | IEC 60754-2 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Head Temperature | 170 | °C |
Flammability | Nominal Value | Unit | Test Method |
---|---|---|---|
Oxygen Index | 34 | % | ASTM D2863 |
Additional Information |
---|
Two different cooling zone are suggested; the first with temperature around 45/55 °C. |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Drying Temperature | 80.0 | °C | |
Drying Time | 3.0 | hr | |
Cylinder Zone 1 Temp. | 110 | °C | |
Cylinder Zone 2 Temp. | 135 | °C | |
Cylinder Zone 3 Temp. | 145 | °C | |
Cylinder Zone 4 Temp. | 160 | °C | |
Die Temperature | 175 | °C |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
Sylvin 86012-66 Clear | Sylvin Technologies Incorporated | PVC, Unspecified | Sylvin |
Nipol® LX426 | Zeon Corporation | Latex | Nipol® |
Boda BDT601P | Chenguang Fluoro & Silicone Elastomers Co., Ltd. | Fluorelastomer | Boda |
Ecodear® V554R10 | Toray Resin Company | PLA | Ecodear® |
Iupilon® HL-3503 | Mitsubishi Engineering-Plastics Corp | PC | Iupilon® |