Category: | TPE , Thermoplastic Elastomer |
Manufacturer: | Teknor Apex Company |
Trademark: | Monprene® |
Fillers: | - |
Ports: | Qinzhou, Shekou, Shanghai, Ningbo |
Delivery Terms | FOB, CIF, DAP, DAT, DDP |
PDF: | YghyUy_Monprene-RG-20140-X-PRELIMINARY-DATA-.pdf ![]() |
PRICE: | Order Products email sales@su-jiao.com |
Message |
---|
Monprene RG-20160 is specifically designed for regulated applications including food contact, toys, and children's products. This grade is suitable for extrusion. Monprene RG-20160 complies with various US FDA and European regulations and directives for food contact and toy safety. Please contact Teknor Apex for a regulatory compliance letter. |
General Information | |
---|---|
Features |
|
Uses |
|
Agency Ratings |
|
Appearance |
|
Forms |
|
Processing Method |
|
Physical | Nominal Value | Unit | Test Method |
---|---|---|---|
Density | 0.890 | g/cm³ | ISO 1183 |
Melt Mass-Flow Rate (MFR) (200°C/5.0 kg) | 0.50 | g/10 min | ASTM D1238 |
Hardness | Nominal Value | Unit | Test Method |
---|---|---|---|
Durometer Hardness (Shore A, 5 sec) | 40 | ISO 868 |
Elastomers | Nominal Value | Unit | Test Method |
---|---|---|---|
Tensile Stress 1 | ISO 37 | ||
Transverse flow : 100% strain | 0.800 | MPa | ISO 37 |
Flow : 100% strain | 2.00 | MPa | ISO 37 |
Tensile Stress 2 | ISO 37 | ||
Transverse flow : Fracture | 6.00 | MPa | ISO 37 |
Flow : Fracture | 2.20 | MPa | ISO 37 |
Tensile Elongation 3 | ISO 37 | ||
Transverse flow : Fracture | 800 | % | ISO 37 |
Flow : Fracture | 140 | % | ISO 37 |
Compression Set 4 | ISO 815 | ||
23°C, 22 hr | 11 | % | ISO 815 |
70°C, 22 hr | 21 | % | ISO 815 |
Fill Analysis | Nominal Value | Unit | Test Method |
---|---|---|---|
Apparent Viscosity (200°C, 206 sec^-1) | 290 | Pa·s | ASTM D3835 |
Extrusion | Nominal Value | Unit | |
---|---|---|---|
Cylinder Zone 1 Temp. | 149 - 160 | °C | |
Cylinder Zone 2 Temp. | 160 - 204 | °C | |
Cylinder Zone 3 Temp. | 171 - 216 | °C | |
Cylinder Zone 4 Temp. | 182 - 227 | °C | |
Die Temperature | 182 - 227 | °C |
Extrusion instructions |
---|
Screw Speed: 30 to 100 rpmDrying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150F (65C). |
Note Message | |
---|---|
1 . | Type 1, 510mm/min |
2 . | Type 1, 510mm/min |
3 . | Type 1, 510mm/min |
4 . | Type a |
Resin Grade | Manufacturer | Category | Trademark |
---|---|---|---|
VESTODUR® 2000 | Evonik Industries AG | PBT | VESTODUR® |
Chiao Fu PA66/6 MB312GM33 BK | Chiao Fu Enterprises Co., Ltd. | Nylon 66/6 | Chiao Fu PA66/6 |
OmniLon™ PA6/6 U IM20 HS BK1000 | OMNI Plastics, LLC | Nylon 66 | OmniLon™ |
POLYFORT® FPP 22 T K1093 | A. Schulman Europe | PP Homopolymer | POLYFORT® |
LNP™ FARADEX™ AX88130 compound | SABIC Innovative Plastics | ABS | LNP™ FARADEX™ |